A vacuum oil purifier, multifunctional technology, applied in separation methods, filtration separation, chemical instruments and methods, etc., can solve the problems of high operating cost, low purification efficiency, complex structure, etc., achieve good results, improve adhesion, High filtering effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0039] As shown in the figure, a multifunctional vacuum oil purifier includes an oil inlet pump, an oil inlet valve, a coarse filter, a heater, a vacuum tank, an oil outlet pump, a fine filter, an oil outlet valve, a condenser, a waste liquid tank, a vacuum pump, Check valve, one end of the oil inlet valve is connected to the oil inlet pump through a pipeline, the other end is connected to the coarse filter through a pipeline, the coarse filter is connected to the heater through a pipeline, the heater is connected to the vacuum tank through a pipeline, and the vacuum tank is connected to the oil outlet pump through a pipeline Pipeline connection, the oil outlet pump is connected to the fine filter through pipelines, the oil outlet pump is connected to the oil outlet valve through pipelines, the vacuum tank is connected to the condenser through pipelines, the lower end of the condenser is connected to the waste liquid tank through pipelines, and the condenser is connected to the ...
Embodiment 2
[0056] It is basically the same as Example 1, the difference is:
[0057] The preparation method of described oil-proof coating is as follows:
[0058]Step (1) Weigh raw materials: by weight, weigh 20 parts of nano-titanium oxide, 20 parts of nano-alumina, 20 parts of nano-silicon oxide, 10 parts of perhydropolysilazane, 5 parts of propylene powder, pulverized coal 5 parts of ash, 5 parts of talcum powder, 10 parts of absolute ethanol, 20 parts of acetone, 30 parts of isopropanol, 10 parts of phenyltrichlorosilane, and 10 parts of silane coupling agent;
[0059] Step (2) Initial mixing: Add nano-titanium oxide, nano-alumina, nano-silicon oxide, dispersant, and organic solvent into the reaction kettle, perform ultrasonic treatment first, and then stir and mix after ultrasonic dispersion. The stirring time is 2 hours, and the stirring temperature is 120°, stirring speed 500r / min;
[0060] Step (3) remixing: Add perhydropolysilazane, filler, and silicone resin into the reaction...
Embodiment 3
[0063] It is basically the same as Example 1, the difference is:
[0064] The preparation method of described oil-proof coating is as follows:
[0065] Step (1) Weigh raw materials: by weight, weigh 10 parts of nano-titanium oxide, 20 parts of nano-alumina, 5 parts of nano-silicon oxide, 5 parts of perhydropolysilazane, 5 parts of propylene powder, kaolin powder 5 parts, 5 parts of fly ash, 5 parts of talcum powder, 10 parts of absolute ethanol, 20 parts of acetone, 30 parts of isopropanol, 10 parts of phenyltrichlorosilane, 10 parts of silane coupling agent;
[0066] Step (2) Initial mixing: Add nano-titanium oxide, nano-alumina, nano-silicon oxide, dispersant, and organic solvent into the reaction kettle, perform ultrasonic treatment first, and then stir and mix after ultrasonic dispersion. Stirring time is 1h, stirring temperature 120°, stirring speed 500r / min;
[0067] Step (3) remixing: Add perhydropolysilazane, filler, and silicone resin into the reaction kettle, stir ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com