Citrate modified up-conversion luminescent nano material and preparation method thereof, hydrogen peroxide or uric acid detection method and applications
A citrate and detection method technology, applied in the direction of luminescent materials, material analysis by optical means, nanotechnology for materials and surface science, etc., can solve the problems of time-consuming and labor-intensive, complicated experimental steps, low sensitivity, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0030] The invention provides a citrate modified NaYF 4 : Yb, the preparation method of Er / Mn up-conversion luminescence nano material, this preparation method comprises:
[0031] 1) Stir alkali, water, oleic acid, C1-C3 alcohol, manganese source, ytterbium source, yttrium source, erbium source and NaF, followed by hydrothermal reaction and centrifugation to obtain OA-NaYF 4 : Yb, Er / Mn UCNPs (NaYF coated with oleic acid 4 : Yb, Er / Mn up-conversion nanomaterial);
[0032] 2) Add OA-NaYF 4 :Yb, Er / Mn UCNPsOA-NaYF 4 : Yb, Er / Mn upconversion nanoparticles dispersed in alcohol, followed by ligand exchange reaction with chloroform and citrate solution to obtain citrate-modified NaYF 4 : Yb, Er / Mn UCNPs upconverting nanoparticles.
[0033] In step 1) of the present invention, the consumption of each material can be selected in a wide range, but in order to improve NaYF 4 : Yb, Er / Mn up-conversion luminescent nanomaterial yield, preparation rate and prepared citrate-modified Na...
Embodiment 1
[0054] 1) OA-NaYF 4 : Yb, Er / Mn up-conversion nanomaterials (OA-NaYF 4 :Yb, the preparation of Er / Mn UCNPs):
[0055] First, weigh 0.300g of NaOH and place it in a 50mL beaker, then add 1.50mL of ultrapure water, 5.00mL of oleic acid, 10.0mL of ethanol, stir well and then add 0.500mL of MnCl 2 solution (0.600mol / L), 1.00mL Y(NO 3 ) 3 solution (0.500mol / L), 0.900mL YbCl 3 solution (0.200mol / L) and 0.100mL Er(NO 3 ) 3 solution (0.200mol / L). Then, 4.00 mL of NaF solution (1.00 mol / L) was added dropwise and stirred gently at 25 °C for 15 min, then transferred to a 50 mL reactor, and reacted at 200 °C for 8 h. After natural cooling to 25°C, centrifuge (10000rmp, centrifuge for 5min), and finally wash repeatedly with ultrapure water and ethanol several times to obtain OA-NaYF 4 : Yb, Er / Mn upconversion nanomaterials.
[0056] 2) Citrate-modified NaYF 4 : Preparation of Yb,Er / Mn up-conversion luminescent nanomaterials:
[0057] 30.0 mg oleic acid-coated NaYF 4 Dissolve Yb...
Embodiment 2
[0059] According to the method of Example 1, citrate-modified NaYF4:Yb, Er / Mn up-conversion luminescent nanomaterial A2 was prepared, except that MnCl 2 The concentration of manganese ions in the solution is 0.4mol / L.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com