Archaistic ceramic art ware made by utilizing magnetite tailing and manufacturing process thereof
A manufacturing process, magnetite technology, applied in the field of antique pottery handicrafts and manufacturing technology, can solve the problems of high porosity and water absorption, no improvement in function, and reduced practicability, etc., to achieve good heat resistance and air permeability, and practical Effects of performance improvement and plasticity improvement
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
specific Embodiment 1
[0024] Antique pottery handicrafts made of magnetite tailings, including pottery body and painted glaze, the weight of pottery body is as follows: 48 parts of magnetite tailings, 36 parts of laterite, 7 parts of spodumene, volcanic stone 9 copies;
[0025] Among them, the magnetite tailings slag is selected from the magnetite tailings slag in the Yangshan mining area of Dehua, and its chemical composition is: Al 2 o 3 5.19%, Fe 2 o 3 12.6%, SiO 2 49.6%, K 2 O 0.8%, Na 2 O 0.5%, CaO 22.7%, MgO 3.4%, I.L 4.3%;
[0026] Among them, the red soil is selected from Longque Village, Sanban, Dehua County, and its chemical composition is: SiO 2 56.8%, Al 2 o 3 22.6%, Fe 2 o 3 6.5%, K 2 O 3.4%, Na 2 O 0.3%, MgO 0.8%, CaO 0.5%, TiO 2 0.9%, I.L8.2%.
[0027] The parts by weight of the painted glaze are as follows: 24 parts of Dehua low-temperature stone, 13 parts of Dehua limestone, 23 parts of borax, 9 parts of boric acid, 11 parts of quartz, 15 parts of kaolin, and ...
specific Embodiment 2
[0035] The manufacturing process of the antique pottery handicraft made by using magnetite tailings is characterized in that, the above-mentioned antique pottery handicrafts made by utilizing magnetite tailings are prepared, and the specific steps are as follows:
[0036] Step 1, weighing according to the raw material components of the pottery body, performing wet ball milling for 18-20 hours to obtain mud;
[0037] Step 2, making the mud prepared in step 1 into the required pottery green body by grouting or pressing;
[0038] Step 3: The pottery body is first biscuit-fired to form a biscuit at a temperature of 850-900°C, and painted on the biscuit with a painted glaze. The painted glaze is weighed according to the raw material components, and the German Low-temperature stone, Dehua limestone, borax and boric acid are made into frit at 1150-1200°C. When painting, the frit is quenched and then added with quartz, kaolin and color materials, and ball milled for 45-50 hours;
[0...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com