Hollow floor mandrel filling body and manufacturing method thereof
A technology of hollow floor and manufacturing method, which is applied to floors, building components, buildings, etc., can solve problems such as low production efficiency and use efficiency, flammability, and affecting building quality, so as to improve product cost performance, reduce material consumption, and lighten The effect of product weight
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0030] A hollow floor mandrel filling body is characterized in that it at least includes the following raw materials: stone powder materials, fiber materials, starch, mold release agent and water.
[0031] The parts by mass of each raw material are: 60-80 parts of stone powder materials, 10-30 parts of fiber materials, 8-12 parts of starch, 0.5-1.5 parts of release agent, and 25-45 parts of water.
[0032] Stone powder materials are one or more of talcum powder, gypsum powder, double fly powder, calcium powder, fly ash, water treatment lime mud or other powdery industrial waste residues.
[0033] The fiber material is one or a mixture of waste paper powder fiber, crop straw fiber and wood powder fiber.
[0034] The starch refers to potato plant starch with high cohesiveness.
[0035] The release agent refers to a powdery or granular industrial release agent with good thermal stability, such as stearic acid, zinc stearate, etc.
[0036] In the filling body of the hollow floor...
Embodiment 2
[0041] In this example, the middle value of the material ratio is taken: 70 parts of stone powder material, 20 parts of fiber material, 10 parts of starch, 1 part of release agent, and 35 parts of water. The hollow floor mandrel filling body made by this ratio See Table 1 for comparison with the existing foam material mandrel filling body, concrete foam mandrel filling body, prefabricated gypsum mandrel filling body, and light steel box mandrel filling body.
[0042] weight cost Structural strength Environmental protection Construction Convenience fire safety Placement labor this invention 10-15 kg 20-30 yuan excellent excellent excellent generally excellent Foam core mold filler 8-12kg 30-40 yuan Difference Difference generally Difference generally Plastic material mandrel filler 10-15 kg 35-45 yuan Difference Difference generally Difference generally Concrete Mandrel Filler 30-40kg 40-50 y...
Embodiment 3
[0045] In this embodiment, the end value of the material ratio is taken: 80 parts of stone powder material, 10 parts of fiber material, 8 parts of starch, 0.5 part of release agent, and 25 parts of water, and the hollow floor mandrel made by the ratio described in this embodiment Compared with the proportion described in Example 2, the strength of the filling body is slightly lower than that of the hollow floor core mold filling body made in Example 2, but it can also meet the industry standard and the cost is lower.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com