A wood floor, anti-fracture technology, applied in coatings, lignin coatings, cellulose coatings, etc., can solve the problems of easy breeding of bacteria, insects, increased probability of breakage, and easy breeding of bacteria, so as to reduce the breeding of bacteria and enhance the Strength, simple effect of preparation method
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
specific Embodiment 1
[0028] Specific embodiment 1: the backside strengthening anti-fracture coating of wooden floor, including the following raw material composition in parts by weight:
[0029] Bottom oil: 150 parts of soybean, 5 parts of monochloroacetic acid, 2 parts of cleaning factor, 12 parts of rapeseed oil, 10 parts of MQ silicone resin, 4 parts of 107 silicone rubber;
[0030] Middle layer particles: 7 parts of talc, 2 parts of cotton linters, 5 parts of resole phenolic resin, 20 parts of boron carbide, 2 parts of modified aliphatic amine curing agent;
[0031] Surface Adhesive: 40 parts of naphthenic base oil, 1 part of hydrochloric acid, 8 parts of amine and polyamide mixture, 8 parts of EVA resin, 6 parts of alkali lignin, 2 parts of sodium hydroxide, 2 parts of 200# dissolved gasoline, polyamide 1 part of amide resin, 3 parts of flower tea.
[0032] Preferably: the raw material composition of the following parts by weight is included:
[0033] Bottom oil: 200 parts of soybean, 10 pa...
specific Embodiment 2
[0041] Specific embodiment 2: the reinforced anti-fracture coating on the back of the wooden floor comprises the following raw materials in parts by weight:
[0042] Bottom oil: 200 parts of soybean, 10 parts of monochloroacetic acid, 5 parts of cleaning factor, 16 parts of rapeseed oil, 12 parts of MQ silicone resin, 5 parts of 107 silicone rubber;
[0043] Middle layer particles: 9 parts of talc, 5 parts of cotton linters, 15 parts of resole phenolic resin, 25 parts of boron carbide, 3 parts of modified aliphatic amine curing agent;
[0044] Surface adhesive: 50 parts of naphthenic base oil, 3 parts of hydrochloric acid, 12 parts of amine and polyamide mixture, 12 parts of EVA resin, 8 parts of alkali lignin, 3 parts of sodium hydroxide, 6 parts of 200# dissolved gasoline, polyamide 2 parts of amide resin, 4 parts of flower tea.
[0045] The preparation method of the reinforced anti-fracture coating on the back of the wooden floor is characterized in that: comprising the fo...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com