Looking for breakthrough ideas for innovation challenges? Try Patsnap Eureka!

Preparation method of high-plugging-strength leaking-stopping agent for well drilling

A technology of plugging agent and high-strength technology, which is applied in the field of preparation of high plugging strength drilling plugging agent, can solve the problems of lower plugging layer permeability, weak water erosion resistance, low plugging strength, etc., and achieve improved plugging High success rate, strong water erosion resistance, and high plugging strength

Inactive Publication Date: 2017-03-22
常州市鼎升环保科技有限公司
View PDF3 Cites 6 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0005] The technical problem mainly solved by the present invention: aiming at the defects that the existing leak-stopping agent has small expansion, weak water erosion resistance, low plugging strength, and easy to cause repeated leakage, it provides a method of using modified cassava starch Graft copolymerization with butyl acrylate, under the action of coupling agent, through maleic anhydride, combined with bamboo fiber, and then adding expanded vermiculite to synthesize the method of high plugging strength drilling plugging agent, the invention first combines tapioca starch and hydrogen peroxide After mixing, stir and react with dodecyl mercaptan, remove the supernatant, react with butyl acrylate and ethylene glycol under nitrogen protection, then add methyl ethyl ketone peroxide to react, remove the ethylene glycol after the reaction, collect the residue and mix with Bamboo fiber, expanded vermiculite, etc. are placed in a high-pressure reactor for reaction, and then cooled and discharged to obtain a plugging agent for drilling with high plugging strength. Methyl ethyl ketone is used as an initiator to graft modified butyl polyacrylate to increase the expansion, and then use maleic anhydride to modify bamboo fiber, and combine it with modified tapioca starch grafted polybutyl acrylate through a coupling agent to increase The principle of adding expanded vermiculite to increase the expansion and plugging strength effectively solves the problem that the existing plugging agent has a small expansion, weak water erosion resistance, low plugging strength, and easy to cause repeated leakage. For the complex formation with large fractures and porous holes, the plugging agent can reduce the permeability of the plugging layer, obtain high plugging layer strength and high pressure bearing capacity of the plugging layer.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

example 1

[0017] First, according to the mass ratio of 1:3, take tapioca starch and hydrogen peroxide with a mass fraction of 20% and put them into a container, put the container in a water bath, set the temperature at 90°C, stir at 130r / min for 4h, and then pour it into the container Add 2% dodecyl mercaptan of cassava starch quality, continue to stir for 10min, then take out the container and let it stand for 2h, remove the supernatant, and collect the residue; then by weight parts, take 50 parts of the above residue, 25 Parts of butyl acrylate, 20 parts of ethylene glycol, 3 parts of methyl ethyl ketone peroxide and 2 parts of ethylene glycol antimony, first put the above residue, butyl acrylate and ethylene glycol into a mixing tank with a stirrer, thermometer and dropping funnel Place the four-necked flask in a water bath, use nitrogen protection, set the temperature at 45°C, and stir at 120r / min for 10min; The methyl ethyl ketone peroxide was added dropwise into the four-necked fl...

example 2

[0020]First, according to the mass ratio of 1:3, take tapioca starch and hydrogen peroxide with a mass fraction of 20% and put them into a container, put the container in a water bath, set the temperature at 97°C, stir at 130r / min for 5h, and then pour it into the container Add 3% dodecyl mercaptan of tapioca starch quality, continue to stir for 13min, then take out the container and let stand for 2h, remove the supernatant, and collect the residue; then in parts by weight, take 55 parts of the residue, 28 21 parts of butyl acrylate, 21 parts of ethylene glycol, 4 parts of methyl ethyl ketone peroxide and 4 parts of ethylene glycol antimony, first put the above residue, butyl acrylate and ethylene glycol into the tank with agitator, thermometer and dropping funnel Place the four-necked flask in a water bath, use nitrogen protection, set the temperature at 48°C, and stir at 120r / min for 13min; The methyl ethyl ketone peroxide was added dropwise into the four-necked flask at 2 d...

example 3

[0023] First, according to the mass ratio of 1:3, take tapioca starch and 20% hydrogen peroxide into the container, put the container in a water bath, set the temperature at 105°C, stir at 130r / min for 6h, and then pour it into the container Add 4% dodecyl mercaptan of tapioca starch quality, continue to stir for 15min, then take out the container and let it stand for 3h, remove the supernatant, and collect the residue; then by weight parts, take 60 parts of the above residue, 30 Parts of butyl acrylate, 22 parts of ethylene glycol, 5 parts of methyl ethyl ketone peroxide and 6 parts of ethylene glycol antimony, first put the above residue, butyl acrylate and ethylene glycol into a tank with a stirrer, thermometer and dropping funnel Place the four-necked flask in a water bath, use nitrogen protection, set the temperature at 50°C, and stir at 120r / min for 15min; The methyl ethyl ketone peroxide was added dropwise into the four-necked flask at 2 drops / s, and at the same time, t...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

PropertyMeasurementUnit
strengthaaaaaaaaaa
Login to View More

Abstract

The invention discloses a preparation method of a high-plugging-strength leaking-stopping agent for well drilling, belonging to the technical field of preparation of leaking-stopping agents. The theory of the preparation method comprises the following steps: carrying out graft modification on butyl polyacrylate resin by utilizing oxidized cassava starch and taking methyl ethyl ketone peroxide as an initiator under the catalysis of ethylene glycol antimony, so as to enhance expansibility; then modifying bamboo fibers by virtue of maleic anhydride, and combining the bamboo fibers with modified cassava starch grafted butyl polyacrylate resin by virtue of a coupling agent, so as to enhance strength; and then adding expanded vermiculite, so as to enhance the swell capacity and plugging strength. By utilizing the theory, the defects of existing leaking-stopping agents that the swell capacity is relatively low, the water flushing resistance is relatively weak, the plugging strength is low, and the repeated leakage easily occurs are effectively solved; and by applying the leaking-stopping agent to complex formations with big crevices and multiple caves, the permeability of a blocked layer can be well decreased, and the high strength and pressure resistance of the blocked layer can be obtained.

Description

technical field [0001] The invention discloses a preparation method of a plugging agent for drilling with high plugging strength, and belongs to the technical field of plugging agent preparation. Background technique [0002] Lost circulation is a common problem in the drilling process, and may cause other downhole complex situations and major accidents such as well collapse, pipe sticking, blowout, etc., which is extremely harmful to drilling work, and may even lead to the scrapping of the wellbore, resulting in huge economic losses. There are dozens of existing plugging technologies, which are mainly divided into bridging plugging materials, high water loss plugging materials, temporary plugging materials, chemical plugging materials, inorganic gel plugging materials, soft and hard plugging materials according to different mechanisms and functions. Plugging materials, high temperature plugging materials, composite plugging materials. [0003] At present, a more effective ...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Applications(China)
IPC IPC(8): C09K8/467C08F251/00C08F220/18
CPCC08F251/00C09K8/426C09K8/467C08F220/1804
Inventor 许斌邹玉薛蕾
Owner 常州市鼎升环保科技有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products