Production method of pure silk quilt with jasmine flower fragrance
A technology of jasmine and mulberry silk, which is applied in applications, non-woven fabrics, household appliances, etc., to achieve the effect of short processing process, easy processing and comfortable mood
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0030] Adopt the following steps to complete the pure mulberry silk quilt with jasmine fragrance:
[0031] (1) Put the cooked silkworms that have been emptied of feces and urine on the silk screen, and the density of cooked silkworms is 850-900 / ㎡;
[0032] (2) After the cooked silkworms have finished spinning, the silk is stripped from the spinning net to obtain a smooth fluffy sheet;
[0033] (3) Scouring with hydrogen peroxide solution with a temperature of 98-100°C and a mass percent concentration of 4% for 35-40 minutes, and degumming the wool sheet until the sericin content is 2.5-2.8%;
[0034] (4) Clean the degummed cotton sheet with clean water, and then place it in a dehydrator for dehydration;
[0035] (5) After the dehydrated cotton sheet is treated with impurity removal and shaping, it is dried to obtain a dry cotton sheet for use; the drying temperature is 65-8 degrees, and the moisture regain is controlled below 12%;
[0036] (6) Jasmine picking reserve: Pick j...
Embodiment 2
[0049] Adopt the following steps to complete the pure mulberry silk quilt with jasmine fragrance:
[0050] (1) Put the cooked silkworms that have been emptied of feces and urine on the silk screen, and the density of cooked silkworms is 800-850 / ㎡;
[0051] (2) After the cooked silkworms have finished spinning, the silk is stripped from the spinning net to obtain a smooth fluffy sheet;
[0052] (3) Scouring with hydrogen peroxide solution with a temperature of 98-100°C and a concentration of 4% by mass for 30-35 minutes, and degumming the wool sheet until the sericin content is 2.8-3.2%;
[0053] (4) Clean the degummed cotton sheet with clean water, and then place it in a dehydrator for dehydration;
[0054] (5) After the dehydrated cotton sheet is treated with impurity removal and shaping, it is dried to obtain a dry cotton sheet for use; the drying temperature is 70-80 degrees, and the moisture regain is controlled below 12%;
[0055] (6) Jasmine picking reserve: Pick jasmine...
Embodiment 3
[0068] Adopt the following steps to complete the pure mulberry silk quilt with jasmine fragrance:
[0069] (1) Put the cooked silkworms that have been emptied of feces and urine on the silk screen, and the density of cooked silkworms is 880-900 / ㎡;
[0070] (2) After the cooked silkworms have finished spinning, the silk is stripped from the spinning net to obtain a smooth fluffy sheet;
[0071] (3) Scouring with hydrogen peroxide solution with a temperature of 98-100°C and a mass percent concentration of 4% for 38-40 minutes, and degumming the wool sheet until the sericin content is 3.2-3.5%;
[0072] (4) Clean the degummed cotton sheet with clean water, and then place it in a dehydrator for dehydration;
[0073] (5) After the dehydrated cotton sheet is treated with impurity removal and shaping, it is dried to obtain a dry cotton sheet for use; the drying temperature is 75-85 degrees, and the moisture regain is controlled below 12%;
[0074] (6) Jasmine picking reserve: Pick ...
PUM
Property | Measurement | Unit |
---|---|---|
width | aaaaa | aaaaa |
thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com