Production method of anti-slip and highlight leatherette paper
A production method and technology of leather-filled paper, applied in paper, papermaking, paper coating, etc., can solve the problems of non-slip resistance, stain resistance and water resistance, unstable items, easy slipping, etc., to reduce lint and powder Phenomenon, excellent sealing performance, effect of improving coating gloss
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0022] The production method of a kind of non-slip high-gloss leather-filled paper proposed by the present invention includes the selection of the original leather-filled backing paper, dipping processing, primary finishing, primer coating, primary top coating, secondary finishing, secondary top coating, and glazing oil, anti-skid varnish and embossing; the first top coating and the second top coating all adopt the method of gravure full plate coating to coat the top coating ink on the paper surface, wherein, the drying temperature is 120 ℃, the vehicle speed It is 20m / min.
Embodiment 2
[0024] The production method of a kind of non-slip high-gloss leather-filled paper proposed by the present invention includes the selection of the original leather-filled backing paper, dipping processing, primary finishing, primer coating, primary top coating, secondary finishing, secondary top coating, and glazing Oil, anti-slip varnish and embossing; the first top coating and the second top coating all adopt the method of gravure full plate coating to coat the top coating ink on the paper; wherein, the drying temperature is 110 °C, and the vehicle speed It is 60m / min.
Embodiment 3
[0026] The production method of a kind of non-slip high-gloss leather-filled paper proposed by the present invention includes the selection of the original leather-filled backing paper, dipping processing, primary finishing, primer coating, primary top coating, secondary finishing, secondary top coating, and glazing oil, anti-slip varnish and embossing; the first top coating and the second top coating all adopt the method of gravure full plate coating to coat the top coating ink on the paper; wherein, the toner content in the top coating ink Accounting for 5wt%, the total absolute dry weight of the top coat paint is 10g, the drying temperature is 118°C, and the vehicle speed is 35m / min;
[0027] Wherein, the selection of the original leather-filled bottom paper is that the selected fiber raw materials and weight ratio are 65% of coniferous wood pulp and 35% of chemical fiber. , and then it is formed by batching, slurry conveying, inclined mesh forming, drying and dehydration, ...
PUM
Property | Measurement | Unit |
---|---|---|
Basis weight | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com