A dyeing method and polar fleece technology, which is applied in the field of dyeing polar fleece fabrics, can solve the problems of poor dyeing uniformity, easy to produce color flowers, and low color fastness of dyed fabrics, and achieve excellent color fastness to light , Optimal dyeing effect, good dyeing uniformity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0039] The dyeing method of polar fleece fabric comprises the steps:
[0040] 1) Add 1 to 2 parts by weight of sodium acetate, 0.9 parts by weight of tetrasodium glutamic acid diacetate, 1.1 parts by weight of γ-glycidyl ether trimethoxysilane, and 2.9 parts by weight of fatty acid polyethylene glycol in the dye vat Add 150 parts by weight of deionized water to the ester and 45 parts by weight of vegetable dyes, stir evenly, and heat to 55°C;
[0041] 2) Add 0.7 parts by weight of powdered sodium carbonate, 2.2 parts by weight of isomeric alcohol polyoxyethylene ether, 0.9 parts by weight of polyoxyethylene fatty amine, 0.4 parts by weight of N-vinylpyrrolidone / acrylamide copolymer, and continue to stir. Mix well and heat to 65°C;
[0042] 3) Soak the fabric in the dye vat for 30 minutes;
[0043] 4) drying the soaked fabric at 80°C;
[0044] 5) Soak the dried fabric in clean water and rinse for 30 minutes;
[0045] 6) Take out the rinsed fabric and let it dry naturally. ...
Embodiment 2
[0047] The dyeing method of polar fleece fabric comprises the steps:
[0048] 1) Add 1 part by weight of sodium acetate, 0.9 parts by weight of tetrasodium glutamic acid diacetate, 1.1 parts by weight of γ-glycidyl ether trimethoxysilane, 2.9 parts by weight of fatty acid polyethylene glycol ester, 45 parts by weight of plant dyes are put into 150 parts by weight of deionized water in turn, stirred evenly, and heated to 55°C;
[0049] 2) Add 0.7 parts by weight of powdered sodium carbonate, 2.2 parts by weight of isomeric alcohol polyoxyethylene ether, 0.9 parts by weight of polyoxyethylene fatty amine, 0.4 parts by weight of N-vinylpyrrolidone / acrylamide copolymer, and continue to stir. Mix well and heat to 65°C;
[0050] 3) Soak the fabric in the dye vat for 30 minutes;
[0051] 4) drying the soaked fabric at 80°C;
[0052] 5) Soak the dried fabric in clean water and rinse for 30 minutes;
[0053] 6) Take out the rinsed fabric and let it dry naturally.
Embodiment 3
[0055] The dyeing method of polar fleece fabric comprises the steps:
[0056] 1) Add 2 parts by weight of sodium acetate, 0.9 parts by weight of tetrasodium glutamic acid diacetate, 1.1 parts by weight of γ-glycidyl ether trimethoxysilane, 2.9 parts by weight of fatty acid polyethylene glycol ester, 45 parts by weight of plant dyes are put into 150 parts by weight of deionized water in turn, stirred evenly, and heated to 55°C;
[0057] 2) Add 0.7 parts by weight of powdered sodium carbonate, 2.2 parts by weight of isomeric alcohol polyoxyethylene ether, 0.9 parts by weight of polyoxyethylene fatty amine, 0.4 parts by weight of N-vinylpyrrolidone / acrylamide copolymer, and continue to stir. Mix well and heat to 65°C;
[0058] 3) Soak the fabric in the dye vat for 30 minutes;
[0059] 4) drying the soaked fabric at 80°C;
[0060] 5) Soak the dried fabric in clean water and rinse for 30 minutes;
[0061] 6) Take out the rinsed fabric and let it dry naturally.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com