A polyester viscose core-spun yarn and process technology, which is applied in the directions of yarn, textile and papermaking, can solve the problems of the quality degradation of polyester-viscose core-spun yarn, loose cohesion of outer fibers, hidden dangers in dyeing and finishing processes, etc., and achieve anti-fuzzing. The effect of spherical improvement, uniform elasticity, reduction of hairiness and broken ends
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0019] Using ordinary polyester medium-long fiber, viscose medium-long fiber, high-strength polyester medium-long fiber, and spandex yarn as raw materials, the polyester medium-long fiber is artificially loosened, and 2wt% of antistatic agent is added to wet and milk. 24 Hours to make it penetrate uniformly and control the moisture regain within 3-5%. The antistatic agent is prepared by making 2wt% sodium alginate aqueous solution from sodium alginate extracted from kelp, and then adding 1wt% mussel mucin to make. The ratio of polyester medium and long fibers: viscose medium and long fibers is 65:35, of which the ratio of ordinary polyester medium and long fibers: high-strength polyester medium and long fibers is 60:5, and the polyester fibers are made by opening, carding, and drawing. Draw frame A, roving, and viscose medium-long fibers are opened and cleared, carded, and drawn to make draw frame B and roving. After roving draw frame A and draw frame B are mixed with spandex y...
Embodiment 2
[0021] Using ordinary polyester medium-long fiber, viscose medium-long fiber, high-strength polyester medium-long fiber, and spandex yarn as raw materials, the ordinary polyester medium-long fiber and high-strength medium-long fiber are mixed, and they are made by blowing, carding, and drawing. Sliver A, roving, and viscose medium-long fibers are opened and cleared, carded, and drawn to make draw B, roving, draw draw A and draw B after roving are mixed into draw C, draw C warp spun yarn , Automatic yarn winding, inspection and packaging, and storage, where the weight ratio of polyester medium and long fibers to viscose medium and long fibers is 65:35, and the weight ratio of ordinary polyester medium and long fibers to high-strength polyester medium and long fibers in drawing A It is 60:5. It is picked up by the cotton machine and sent to the opener. The three-wing needle beater is used. The beater speed is 500r / min. The distance between the beater and the dust bar in the opener...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com