Negative oxygen environment-friendly color putty
An environmentally friendly and negative oxygen technology, applied in the field of building decoration materials, can solve the problems of single function, unenvironmental protection, uneven paint quality, user health hazards, etc., to achieve the effect of bright and stable colors, stable performance, and optimized environment
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0040] A negative oxygen environment-friendly colored putty, the amount of each component is 40 parts of shell powder passed through a 300-mesh sieve, 10 parts of aluminum silicate fiber, 0.5 part of sodium bentonite, 2 parts of negative ion powder, 15 parts of binder, and isothiazolinone 0.3 parts of quasi-compound, 60 parts of color particles, 2 parts of polyethylene low molecular weight wax, 2 parts of β-hydroxyalkylamide, and 1 part of BYK-019 defoamer.
[0041] Mix water and putty powder according to the mass ratio of 0.4:1. First add water to the container, then gradually add the powder, stir with an electric stirring rod, and put the evenly stirred paste putty for 20-30 minutes. use.
Embodiment 2
[0043] A negative oxygen environment-friendly colored putty, the amount of each component is 50 parts of shell powder passed through a 300-mesh sieve, 15 parts of aluminum silicate fiber, 1 part of sodium bentonite, 5 parts of negative ion powder, 20 parts of binder, and isothiazolinone 0.1 part of paraffin compound, 85 parts of color particles, 5 parts of polyethylene low molecular weight wax, 2 parts of β hydroxyalkylamide, 0.5 part of BYK-019 defoamer.
[0044] Mix water and putty powder according to the mass ratio of 0.4:1. First add water to the container, then gradually add the powder, stir with an electric stirring rod, and put the evenly stirred paste putty for 20-30 minutes. use.
Embodiment 3
[0046] A negative oxygen environment-friendly colored putty, the amount of each component is 65 parts of shell powder passed through a 300-mesh sieve, 15 parts of aluminum silicate fiber, 0.8 part of sodium bentonite, 8 parts of negative ion powder, 25 parts of binder, and isothiazolinone 1 part of paraffin compound, 75 parts of color particles, 3 parts of polyethylene low molecular weight wax, 3 parts of β hydroxyalkylamide, 2 parts of BYK-019 defoamer.
[0047] Mix water and putty powder according to the mass ratio of 0.5:1. First add water to the container, then gradually add the powder, stir with an electric stirring rod, and put the evenly stirred paste putty for 20-30 minutes. use.
[0048] Before construction, oil stains, floating ash, dirt and other substances on the surface of the substrate should be removed to ensure that the surface of the substrate is clean. In order to avoid the surface of the substrate being too dry and causing water absorption to the putty on th...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com