Method for preparing coarse aggregates from coral reefs and concrete
A coral reef and concrete technology, which is applied in the field of preparing coarse aggregate and concrete by using coral reef, can solve the problems of insufficient concrete strength, unstable work performance, early setting of seawater and sea sand concrete, etc., to protect mines and forestry resources, The effect of promoting ecological environment protection and huge social and economic benefits
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0034] The present embodiment provides a kind of method utilizing coral reef to prepare coarse aggregate, comprising the following steps: (1) washing coral reef with seawater, then immersing the washed coral reef with 0.4mol / L hydrochloric acid for 8h, and then washing with seawater Remove residual hydrochloric acid on the surface of the coral reef; (2) pass the coral reef soaked in hydrochloric acid through a 5mm square hole sieve to obtain a sieve residue; (3) soak the sieve residue with 5% water glass solution for 10 hours Take it out and get coarse aggregate after drying in the sun.
Embodiment 2
[0036] The present embodiment provides a kind of method utilizing coral reef to prepare coarse aggregate, comprising the following steps: (1) washing coral reef with seawater, then immersing the washed coral reef with 0.8mol / L hydrochloric acid for 4h, and then cleaning with seawater Remove residual hydrochloric acid on the surface of the coral reef; (2) pass the coral reef soaked in hydrochloric acid through a 5mm square hole sieve to obtain a sieve residue; (3) soak the sieve residue with 10% water glass solution for 15 hours Take it out and get coarse aggregate after drying in the sun.
Embodiment 3
[0038] The present embodiment provides a kind of method utilizing coral reef to prepare coarse aggregate, comprising the following steps: (1) washing coral reef with seawater, then immersing the washed coral reef with 0.6mol / L hydrochloric acid for 6h, and then cleaning with seawater Remove the residual hydrochloric acid on the surface of the coral reef; (2) pass the coral reef soaked in hydrochloric acid through a 5mm square hole sieve to obtain a sieve residue; (3) soak the sieve residue with 20% water glass solution for 12 hours Take it out and get coarse aggregate after drying in the sun.
PUM
Property | Measurement | Unit |
---|---|---|
pore size | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com