File ballpoint pen writing protecting agent and protecting method
A technology of ballpoint pen and protective agent, which is applied in the direction of biocide-containing paint, coating, antifouling/underwater coating, etc., can solve the problems of human body damage, volatile, flammable, etc., achieve enhanced mechanical strength, and facilitate industrial production , the effect of simple materials
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0020] Dissolve 6 parts by weight of sodium alginate in 90 parts by weight of water at 70°C, stir while adding, after dissolving evenly, then add 3 parts by weight of glycerin and 1.5 parts by weight of ammonium persulfate, stir evenly, and cool to room temperature Made into A component;
[0021] 8 parts by weight of calcium chloride and 97 parts by weight of water were uniformly mixed to prepare component B. An archival ballpoint pen handwriting protection agent of the present invention is composed of component A and component B.
[0022] When protecting the handwriting of the ballpoint pen in the file, operate as follows:
[0023] (1) Hold the absorbent cotton with tweezers, dip in component A, evenly spread it on the writing of the file ballpoint pen, and dry it with a hair dryer;
[0024] (2) Hold the absorbent cotton with tweezers, dip in component B, evenly spread it on the file ballpoint pen writing in step (1), and dry it with a hair dryer.
Embodiment 2
[0026] Dissolve 8 parts by weight of sodium alginate in 99 parts by weight of water at 80°C and stir while adding. After dissolving evenly, add 5 parts by weight of glycerin and 2 parts by weight of ammonium persulfate in sequence, stir evenly, and cool to room temperature Made into A component;
[0027] 1 part by weight of calcium chloride and 99 parts by weight of water are uniformly mixed to prepare component B.
Embodiment 3
[0029] Dissolve 2 parts by weight of sodium alginate in 95 parts by weight of water at 65°C and stir while adding. After dissolving evenly, add 0.5 parts by weight of glycerin and 0.5 parts by weight of ammonium persulfate in sequence, stir evenly, and cool to room temperature Made into A component;
[0030] 10 parts by weight of calcium chloride and 99 parts by weight of water are uniformly mixed to prepare component B.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com