A sandstone reservoir, retarded acid technology, applied in the direction of chemical instruments and methods, drilling compositions, etc., can solve the problems of fast reaction speed of acid rock, weak retarded acidity, limited dissolution ability, etc., to achieve delayed reaction The effect of speed, unblocking formation, and strong dissolution ability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0020] (1) Weigh 100g of β-cyclodextrin, put it into a mortar, add 30ml of distilled water, and grind until it becomes a paste;
[0021] (2) Weigh 12.7g of methanesulfonic acid powder and add it to the above-mentioned β-cyclodextrin paste;
[0022] (3) Grind the mixture for 2 hours to obtain a uniform paste;
[0023] (4) Put the paste in a drying oven and keep the temperature at 50°C for 12 hours to obtain the inclusion compound of methanesulfonic acid and β-cyclodextrin;
[0024] (5) Add the prepared clathrate and 13.05g of ammonium fluoride into 100ml of water, and stir well until the solid powder is completely dissolved to obtain a high-temperature sandstone reservoir retarded acid solution.
Embodiment 2
[0026] (1) Weigh 113.5g of β-cyclodextrin, put it into a mortar, add 40ml of distilled water, and grind until it becomes a paste;
[0027] (2) Weigh 9.61g of methanesulfonic acid powder and add it to the above-mentioned β-cyclodextrin paste;
[0028] (3) Grind the mixture for 1.5 hours to obtain a uniform paste;
[0029] (4) Put the paste in a drying oven and keep the temperature at 50°C for 8 hours to obtain the inclusion complex of methanesulfonic acid and β-cyclodextrin;
[0030] (5) Add the prepared clathrate and 11.4g of ammonium fluoride into 90ml of water, and stir well until the solid powder is completely dissolved to obtain a high-temperature sandstone reservoir tardy acid solution.
Embodiment 3
[0032] (1) Weigh 113.5g of β-cyclodextrin, put it into a mortar, add 50ml of distilled water, and grind until it becomes a paste;
[0033] (2) Weigh 19.22g of methanesulfonic acid powder and add it to the above-mentioned β-cyclodextrin paste;
[0034] (3) Grind the mixture for 2 hours to obtain a uniform paste;
[0035] (4) Put the paste in a drying oven and keep the temperature at 50°C for 12 hours to obtain the inclusion compound of methanesulfonic acid and β-cyclodextrin;
[0036] (5) Add the prepared clathrate and 45.6g of ammonium fluoride into 60ml of water and stir well until the solid powder is completely dissolved to obtain a high-temperature sandstone reservoir tardy acid solution.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com