A bisoprolol and packaging technology, applied in the field of bisoprolol-containing patch and its packaging, can solve the problems of no revelation, no revelation, stability of bisoprolol over time, etc., and achieve usability and portability Excellent, improved stability and reliability over time, and improved economical efficiency
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0096] 15.1 parts of high molecular weight polyisobutylene (viscosity average molecular weight = 4,000,000), 26.1 parts of medium molecular weight polyisobutylene (viscosity average molecular weight = 55,000), 27.4 parts of alicyclic saturated hydrocarbon resin (tackifier), isopropyl myristate ( 30.0 parts of organic liquid components) and 1.4 parts of bisoprolol (free body) were mixed in toluene to prepare a viscous toluene solution of the adhesive composition. The obtained solution was coated on a polyethylene terephthalate (PET) release liner (thickness: 75 μm) so that the thickness after drying was 160 μm, and it was dried in a hot air circulation dryer. Drying was carried out at 100° C. for 5 minutes to form an adhesive layer.
[0097] The pressure-sensitive adhesive layer was bonded to a PET film and a PET nonwoven fabric (weight per unit area=12 g / m2) having a thickness of 2 μm. 2 ) The non-woven side of the support of the laminated film, punched into 36cm 2 (6 cm x 6...
Embodiment 2
[0101] Under an inert gas atmosphere, make 70.0 parts of 2-ethylhexyl acrylate, 5.0 parts of hydroxyethylacrylamide, 25.0 parts of N-vinyl-2-pyrrolidone, and 0.2 parts of azobisisobutyronitrile as a polymerization initiator in Solution polymerization was carried out at 60°C in ethyl acetate to prepare an acrylic adhesive solution. 65.0 parts of this acrylic adhesive solution, 30.0 parts of isopropyl myristate as an organic liquid component, and 5.0 parts of bisoprolol (free body) were mixed to prepare a viscous ethyl acetate of an adhesive composition. solution. The obtained solution was coated on a polyethylene terephthalate (PET) release liner (thickness 75 μm) so that the thickness after drying was 45 μm, and it was dried in a hot air circulation dryer at 100 °C for 5 minutes to form an adhesive layer.
[0102] The pressure-sensitive adhesive layer was bonded to a PET film and a PET nonwoven fabric (weight per unit area=12 g / m2) having a thickness of 2 μm. 2 ) on the non...
PUM
Property | Measurement | Unit |
---|---|---|
Thickness | aaaaa | aaaaa |
Thickness | aaaaa | aaaaa |
Thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com