Embodiment 1
[0018] The perm agent provided by the present embodiment is made up of the following raw materials in weight percentage:
[0019]
[0020] The preparation method is as follows: weigh the above-mentioned raw materials in proportion respectively, then put 5kg of L-cysteine hydrochloride monohydrate into a container, add 44.95kg of pure water, stir evenly, then slowly add 3kg of ethanolamine and continuously Stir, control the pH at 9.4, and control the temperature at ≤40°C. After the mixture drops to room temperature, add 1kg of urea, stir to dissolve it completely, then add 1kg of glycerol, stir evenly, and then add 0.05kg of water-soluble lanolin successively , 0.05kg water-soluble silicone oil and remaining 44.95kg pure water, constantly stir therebetween, make the described permanent hair agent of 100kg thus.
Embodiment 2
[0022] The perm agent provided by the present embodiment is made up of the following raw materials in weight percentage:
[0023]
[0024]
[0025] The preparation method is as follows: weigh the above-mentioned raw materials in proportion, then put 8kg of L-cysteine hydrochloride monohydrate into a container, add 40.2kg of pure water, stir evenly, then slowly add 5kg of ethanolamine and continuously Stir, control the pH at 9.4, and control the temperature at ≤40°C. After the mixture drops to room temperature, add 3kg of urea, stir to dissolve it completely, then add 3kg of glycerol, stir evenly, and then add 0.15kg of water-soluble lanolin successively , 0.25kg water-soluble silicone oil, 0.2kg essence and remaining 40.2kg pure water, constantly stir therebetween, thus make the described perm agent of 100kg.
Embodiment 3
[0027] The perm agent provided by the present embodiment is made up of the following raw materials in weight percentage:
[0028]
[0029]
[0030] The preparation method is as follows: weigh the above-mentioned raw materials in proportion respectively, then put 11kg of L-cysteine hydrochloride monohydrate into a container, add 35.1kg of pure water, stir evenly, then slowly add 8kg of ethanolamine and continuously Stir, control the pH at 9.4, and control the temperature at ≤40°C. After the mixture drops to room temperature, add 5kg of urea, stir to dissolve it completely, then add 5kg of glycerol, stir evenly, and then add 0.3kg of water-soluble lanolin successively , 0.4kg water-soluble silicone oil, 0.1kg essence and remaining 35.1kg pure water, constantly stir therebetween, thus make the described perm agent of 100kg.
[0031] The hair perm provided by the invention is used in the same way as the currently commonly used hair perm.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com