A technology for rubber products and packers, applied in the field of rubber product preparation, can solve the problems of high temperature resistance, poor high pressure resistance, reduced work efficiency, increased labor and other problems, and achieves excellent oil resistance, increased volume and quality, and reduced The effect of production costs
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0021] A kind of preparation method for the rubber product of packer, comprises the following steps:
[0022] a. Put 23 type fluorine rubber into the double-roller mill, then add reinforcing filler, zinc oxide, magnesium oxide, accelerator DM, epoxy plasticizer, anti-aging agent NBC and vulcanizing agent BP in sequence for mixing 250-350S, the temperature is maintained at 80°C to 100°C to obtain mixture A; the reinforcing filler is a combination of one or more of white carbon black, mica powder and fine particle calcium carbonate;
[0023] b. Add the softener fatty acid glyceride to the mixture A obtained in step a, and then knead for 200~300s to obtain the mixture B;
[0024] c. Put the mixture B obtained in step b into a mould, heat and form it, the heating temperature is 120°C-180°C, and the heating time is 600-900s, and the rubber product for the packer is obtained.
Embodiment 2
[0026] A kind of preparation method for the rubber product of packer, comprises the following steps:
[0027] a. Put 23 type fluorine rubber into the double-roller mill, then add reinforcing filler, zinc oxide, magnesium oxide, accelerator DM, epoxy plasticizer, anti-aging agent NBC and vulcanizing agent BP in sequence for mixing 250-300S, the temperature is kept at 90°C~100°C to obtain mixture A; the reinforcing filler is a mixture of white carbon black and mica powder;
[0028] b. Add softener fatty acid glyceride to mixture A obtained in step a, and then knead for 200~250s to obtain mixture B;
[0029] c. Put the mixture B obtained in step b into a mold, heat and form it, the heating temperature is 120°C-150°C, and the heating time is 600-800s, and the rubber product for the packer is obtained.
Embodiment 3
[0031] A kind of preparation method for the rubber product of packer, comprises the following steps:
[0032] a. Put 23 type fluorine rubber into the double-roller mill, then add reinforcing filler, zinc oxide, magnesium oxide, accelerator DM, epoxy plasticizer, anti-aging agent NBC and vulcanizing agent BP in sequence for mixing 300-350S, the temperature is maintained at 80°C to 90°C to obtain mixture A; the reinforcing filler is a mixture of white carbon black and fine particle calcium carbonate;
[0033] b. Add softener fatty acid glyceride to mixture A obtained in step a, and then knead for 250~300s to obtain mixture B;
[0034] c. Put the mixture B obtained in step b into a mould, heat and shape it, the heating temperature is 150°C-180°C, and the heating time is 700-900s, and the rubber product for the packer is obtained.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com