[0020] Embodiment one: press CaO 40%, SiO 2 30%, MgO 10%, and other elements 20%. Choose one or more of calcareous raw materials; choose one or more of magnesia raw materials; choose one or more of siliceous raw materials, choose flux minerals One or several kinds of ingredients, the standard deviation is controlled at 1%, and then the raw meal is prepared, and its fineness exceeds 100 mesh and enters the raw meal homogenization warehouse. When the degree of homogenization reaches the standard and the deviation is not greater than 0.2%, the The firing temperature is controlled at 1150-1250°C, and the firing time is controlled at 8 hours. After leaving the kiln and cooling sufficiently, it is put into the workshop for grinding. The fineness is over 100 mesh. When the temperature is less than 40°C and the standard deviation is less than 0.2%, it can be packed in 50kg, 40kg, or 25kg for storage.
Embodiment 2
[0022] According to CaO 60%, SiO 2 20%, MgO 5%, and other elements 15%. Choose one or more of the calcareous raw materials, choose one or more of the magnesia raw materials; choose one or more of the siliceous raw materials, choose one or more of the flux minerals One or several kinds of ingredients, the standard deviation is controlled at 1%, and then the raw meal is prepared, and its fineness exceeds 100 mesh and enters the raw meal homogenization warehouse. When the degree of homogenization reaches the standard and the deviation is not greater than 0.2%, the Fired in a rotary kiln, the firing temperature is controlled at 1150 to 1250 ° C, and the firing time is controlled at 0.5 hours. After leaving the kiln and cooling sufficiently, it is put into the workshop for grinding. The fineness is over 100 mesh. After cooling, For homogenization, when the temperature is less than 40°C and the standard deviation is less than 0.2%, it can be packed in 50kg, 40kg, or 25kg for storage...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com