An artificial stone slab and anti-fouling technology, which is applied in the field of clay or stone, and processed cement, can solve the problems of poor anti-pollution ability, and achieve the effects of enhanced anti-fouling performance, excellent self-cleaning ability, and good adsorption capacity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0022] A method for manufacturing a stain-resistant artificial quartz stone, comprising the following steps:
[0023] (1) Evenly mix quartz sand and quartz stone powder, quartz sand: 2 mesh < particle size ≤ 4 mesh, 4 mesh < particle size ≤ 6 mesh, 6 mesh < particle size ≤ 8 mesh, 8 mesh < particle size ≤ 16 mesh, 16 mesh < Grain size ≤ 24 mesh, 24 mesh < particle size ≤ 40 mesh, 40 mesh < particle size ≤ 80 mesh and 80 mesh < particle size ≤ 120, 8 kinds of these 8 kinds of particle gradation accounts for 10%, 10%, 10% of the total weight , 10%, 15%, 15%, 12%; quartz powder 400 mesh ≤ particle size: 6%; accounting for 88% of the total mass.
[0024] (2) Vacuum vibration high-pressure molding: Add 2.3wt% of anti-fouling active factor (1.8wt% white cement, 0.5wt% active factor powder additive) and stir well, then add 1.0wt% water, and stir again, modified resin resin 8.7 Wt% (8wt% vinyl resin, 0.7wt% tetrafluoroethylene-based fluorosilicone resin), after mixing evenly, use a p...
Embodiment 2
[0027] A method for manufacturing a stain-resistant artificial quartz stone, comprising the following steps:
[0028] (1) Evenly mix quartz sand and quartz powder, quartz sand: 2 mesh < particle size ≤ 4 mesh, 4 mesh < particle size ≤ 6 mesh, 6 mesh < particle size ≤ 8 mesh, 8 mesh < particle size ≤ 16 mesh, 16 mesh < Grain size ≤ 24 mesh, 24 mesh < particle size ≤ 40 mesh, 40 mesh < particle size ≤ 80 mesh and 80 mesh < particle size ≤ 120, 8 kinds of these 8 kinds of particle gradation accounted for 12%, 13%, 15% of the total weight in sequence , 10%, 10%, 10%, 10%; quartz powder 400 mesh: 8.6%; accounting for 88.6% of the total mass.
[0029] (2) Vacuum vibration high-pressure molding: add 1.8wt% antifouling active factor (white cement 1.5wt% active factor powder additive 0.3wt%) and stir well, after mixing evenly, add 0.6wt% water, and stir again, then Add 9.0wt% modified resin resin (8wt% vinyl resin, 1wt% tetrafluoroethylene-based fluorosilicone resin), and use a press ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com