Standing modified timber, standing timber modifier, and preparation methods thereof
A technology of living trees and modifiers, which is applied in the fields of botany equipment and methods, gardening methods, gardening tools/equipment, etc. It can solve the problems of affecting the mechanical properties of modified wood, reducing the mechanical properties of wood, and polluting the environment by modifiers , to achieve the effects of easy large-scale popularization and application, simple and easy operation, and no pollution to the environment
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0025] The invention provides a kind of preparation method of standing modified wood, comprising the following steps:
[0026] 1) Select live standing trees with a tree age of more than 6 years and a trunk diameter of 16 to 20 cm;
[0027] 2) At the place where the trunk of the living tree is 20-50cm above the ground, drill holes vertically to the trunk, straight to the pith center of the trunk, the diameter of the holes is 10-30mm, and the number is 6-12, and the holes are evenly distributed along the circumference of the trunk ;
[0028] 3) insert the pipeline into the hole drilled in step 2), inject modifier through the pipeline, and the other end of the pipeline is connected with the container containing the modifier, wherein the container of the modifier is 30cm higher than the hole, and is higher than the crown of the tree. Low; with this injection method, the injection of the agent can be completed without large-scale equipment, and it has the advantages of simple oper...
Embodiment 1
[0037] Choose the fast-growing poplar whose tree age is 6 years and whose trunk diameter is 16cm. At its growth height of 20cm and 40cm from the ground, respectively drill 12 holes with a diameter of 10mm vertically to the trunk. distribution; then insert the pipeline used to inject the nano-phenolic resin composite material, that is, the modifier, and the other end of the pipeline is connected with the container filled with the nano-phenolic resin composite material. Flow, permeate and diffuse to the whole standing tree, and after 2 days, the modification of the standing tree is completed by cutting down. Wherein the nano-phenolic resin composite material container should be close to the standing tree, and should be 30cm higher than the hole and lower than the tree crown, and a shelf should be used to carry the container.
Embodiment 2
[0039] Choose the fast-growing poplar whose tree age is 10 years and whose trunk diameter is 20cm. At its growth height of 30cm and 50cm from the ground, respectively drill 6 holes with a diameter of 30mm vertically to the trunk, straight to the trunk pith center, and the holes are uniform along the trunk circumference. distribution; then insert the pipeline used to inject the nano-phenolic resin composite material, that is, the modifier, and the other end of the pipeline is connected with the container filled with the nano-phenolic resin composite material. Flow, permeate and diffuse to the whole standing tree, and after 4 days, the modification of the standing tree is completed by cutting down. Wherein the nano-phenolic resin composite material container should be close to the standing tree, and should be 30cm higher than the hole and lower than the tree crown, and a shelf should be used to carry the container.
PUM
Property | Measurement | Unit |
---|---|---|
Viscosity | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com