Preparation method for welded steel pipe for boiler
A technology for welding steel pipes and boilers, which is applied in the field of preparing welded steel pipes for boilers, and achieves the effects of high internal and external surface quality, easy operation and good product quality.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0012] A method for preparing welded steel pipes for boilers, comprising the following steps: billet anti-rolling, slitting, forming, welding, deburring, weld heat treatment, sizing, non-oxidizing heat treatment, shaping, flaw detection, cutting, cutting and flattening, coating layers, packaging;
[0013] (1) Billet steel coil: the billet is low-carbon steel, and its composition includes: C 0.11, Si 0.08, Mn 0.45, P≤0.01, S≤0.002, Cr 0.55, Ni 0.03, Nb 0.21, Cu 0.25, Al 0.03 , the rest are Fe and non-metallic impurities; place the above steel billet on the uncoiler for uncoiling;
[0014] (2) Slitting: After slitting, cut off the edge of the billet by 2 to 3mm to prevent the edge of the billet from being damaged during the slitting and lifting process, resulting in some tiny cracks and indentations that cannot be seen clearly with the naked eye, causing safety hazards;
[0015] (3) Forming: through multi-pass forming die extrusion, the steel billet roll is extruded into a tubu...
Embodiment 1
[0028] Process welded steel pipes for boilers with an outer diameter of 51.5mm and a thickness of 3.15mm
[0029] (1) Billet steel coil: low-carbon steel billet with a width of 230mm and a thickness of 3.15mm is selected, and its composition includes: C 0.11, Si 0.08, Mn 0.45, P≤0.01, S≤0.002, Cr 0.55, Ni 0.03, Nb 0.21 , Cu 0.25, Al 0.03, and the rest are Fe and non-metallic impurities; place the above billet on the uncoiler for uncoiling;
[0030] (2) Longitudinal cutting: cut off the edge of the billet by 2 to 3 mm during longitudinal cutting;
[0031] (3) Forming: On the pipe making machine, it is formed into a pipe shape through a double-radius hole forming die, and a straight line weld is left;
[0032] (4) Welding: The welding temperature is 1480°C, and the welding pressure is 32.5MPa;
[0033] (5) Deburring: Use a special disc cutter to remove the burrs inside and outside the welded steel pipe, and the residual height after removal is 0.05mm;
[0034] (6) Weld seam h...
PUM
Property | Measurement | Unit |
---|---|---|
thickness | aaaaa | aaaaa |
thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com