Graphene-based nano zero-valent cobalt-iron-copper lubricating oil and preparation method thereof
A graphene-based, nano-zero-valent technology, used in the petroleum industry, lubricating compositions, additives, etc., can solve the problems of nano-metal ultra-fine particle dispersibility, stability and easy oxidation, and achieve excellent anti-friction and anti-wear effects, excellent Effects of mechanical and electrical properties, high reactivity and selectivity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0027] Take 0.1g of graphene-based nano-zero-valent cobalt, 0.2g of graphene-based nano-zero-valent iron, 0.2g of graphene-based nano-zero-valent copper, 0.2g of graphene-based nano-titanium dioxide, 0.2g of graphene-based nano-potassium borate, diethyl Copper phenylhexyl dithiophosphate 0.3g, polymethacrylate 1.5g, sodium dodecylbenzenesulfonate 1.5g, simethicone 0.02g, rust inhibitor 0.5g, pour point depressant 0.10g, viscosity increaser Add 3.5g of detergent, 0.1g of detergent, and 0.1g of demulsifier. Add 90.0g of synthetic base oil under the condition of electric stirring at 1500rpm at room temperature. After the addition, ultrasonic for 30min to achieve uniform dispersion.
Embodiment 2
[0029] Take 0.2g of graphene-based nano-zero-valent cobalt, 0.1g of graphene-based nano-zero-valent iron, 0.2g of graphene-based nano-zero-valent copper, 0.2g of graphene-based nano-titanium dioxide, 0.2g of graphene-based nano-potassium borate, diethyl Copper phenylhexyl dithiophosphate 0.3g, polymethacrylate 1.5g, sodium dodecylbenzenesulfonate 1.5g, simethicone 0.02g, rust inhibitor 0.5g, pour point depressant 0.10g, viscosity increaser Add 3.5g of detergent, 0.1g of detergent, and 0.1g of demulsifier. Add 90.0g of synthetic base oil under the condition of electric stirring at 1500rpm at room temperature. After the addition, ultrasonic for 30min to achieve uniform dispersion.
Embodiment 3
[0031] Take 0.2g of graphene-based nano-zero-valent cobalt, 0.2g of graphene-based nano-zero-valent iron, 0.2g of graphene-based nano-zero-valent copper, 0.1g of graphene-based nano-titanium dioxide, 0.3g of graphene-based nano-potassium borate, diethyl Copper phenylhexyl dithiophosphate 0.3g, polymethacrylate 1.5g, sodium dodecylbenzenesulfonate 1.5g, simethicone 0.02g, rust inhibitor 0.5g, pour point depressant 0.10g, viscosity increaser Add 3.5g of detergent, 0.1g of detergent, and 0.1g of demulsifier. Add 90.0g of synthetic base oil under the condition of electric stirring at 1500rpm at room temperature. After the addition, ultrasonic for 30min to achieve uniform dispersion.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com