A production method and a technology of polishing bricks, which are applied in the field of architectural ceramics, can solve problems such as the inability to control the distribution of flashing spots on the surface of finished products, the monotonous decoration of patterns on the surface of mechanical fabrics, and the inability to achieve color gradient effects, etc., to achieve diversified decoration methods and delicate decorative patterns. , various layers of effects
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] [Example 1] The production method of glazed porcelain polished tiles of the present invention comprises the following steps:
[0024] 1) Preparation of ordinary porcelain tile formula powder;
[0025] 2) Pattern formation
[0026] ① It is formed by large-grain cloth of porcelain polished tiles;
[0027] ② Inkjet printing pattern with ceramic digital inkjet machine in cooperation with step ①;
[0028] 3) Apply transparent glaze: glaze thickness 0.5mm;
[0029] 4) Firing: The firing temperature is 1150°C, and the firing cycle is 60 minutes;
Embodiment 2
[0031] [Example 2] The production method of glazed porcelain polished tiles of the present invention comprises the following steps:
[0032] 1) Preparation of ordinary porcelain tile formula powder;
[0033] 2) Pattern formation
[0034] ① Formed with porcelain polished brick micro-powder cloth;
[0035] ② Rubber roller printing pattern matched with step ①;
[0036] 3) Apply transparent glaze: glaze thickness 0.7mm;
[0037] 4) Firing: The firing temperature is 1180°C, and the firing cycle is 55 minutes;
Embodiment 3
[0039] [Example 3] The production method of glazed porcelain polished tiles of the present invention comprises the following steps:
[0040] 1) Preparation of ordinary porcelain tile formula powder;
[0041] 2) Pattern formation
[0042] ① It is formed by multi-tube cloth of porcelain polished tiles;
[0043] ② screen printing pattern matched with step ①;
[0044] 3) Apply transparent glaze: glaze thickness 1.0mm;
[0045] 4) Firing: The firing temperature is 1200°C, and the firing cycle is 45 minutes;
[0046] 5) Edge grinding and polishing.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com