A technology of coating urea and humic acid, which is applied in the fields of agricultural gas emission reduction, fertilizer mixture, fertilization equipment, etc., can solve the problem of large-scale production and sales of humic acid-coated urea products, the inability to carry out subsequent processing, and the difficulty of large-scale production. Large-scale production and other issues, to achieve the effect of abundant reserves, improved urea utilization rate, and easy promotion
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0075] Urea specifications: particle size 2.00 ~ 4.75 mm,
[0076] Adhesive composition:
[0077] Styrene-acrylic waterproof emulsion (45%): 75 parts by weight, polyvinyl formal resin (8%): 10 parts by weight, yellow dextrin: 5 parts by weight, water: 10 parts by weight.
[0079] Humic acid (180-300 mesh): 45 parts by weight, sodium humate (120-200 mesh): 15 parts by weight, hemihydrate gypsum (180-300 mesh): 20 parts by weight, calcined diatomite (180-325 mesh ): 8 parts by weight, sodium-based pentonite (160-200 mesh): 4 parts by weight, sodium polyacrylate (160-200 mesh): 6 parts by weight, dicyandiamide (160-200 mesh): 2.0 parts by weight.
[0080] Urea consumption: 90KG
[0081] Adhesive dosage: 1.5KG
[0082] Package powder consumption: 8.5KG
[0083] Follow the steps below:
[0084] (1) Put the binder raw material into the blending tank, mix it with water, and make the binder for subsequent use;
[0085] (2) Mixing humic acid and ...
Embodiment 2
[0091] The urea specification, binder composition, package powder proportioning are the same as embodiment 1
[0092] Urea consumption: 86KG
[0093] Adhesive dosage: 2.0-KG
[0094] Package powder consumption: 12.0KG
[0095] According to embodiment 1 step operation
[0096] After testing, the relative loss control rate of the obtained humic acid-coated urea is 76%, the relative water retention rate is 77%, and the slow dissolution rate is 4.3 times.
Embodiment 3
[0098] The urea specification, binder composition, package powder proportioning are the same as embodiment 1
[0099] Urea consumption: 82KG
[0100] Adhesive dosage: 2.5KG
[0101] Package powder consumption: 15.5KG
[0102] According to embodiment 1 step operation
[0103] After testing, the relative loss control rate of the obtained humic acid-coated urea is 86%, the relative water retention rate is 82%, and the slow dissolution rate is 5.1 times.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com