Preparation method of nanopore cellular membrane
A technology of honeycomb membrane and nanopore, applied in the field of material chemistry
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Benefits of technology
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0014] The preparation method of the nanoporous honeycomb membrane is: select a suitable solvent, configure a polymer solution with a concentration of 6 mg / mL ~ 14 mg / mL; coat the polymer solution on the surface of the substrate, and place it in a place with a relative humidity of 60%~ In 90% normal temperature atmospheric environment, let it stand for 30 seconds to 4 minutes, and after the solvent is completely volatilized, a honeycomb film with a nanopore structure is prepared, and the pore size range is 10 nanometers to 100 nanometers; the solvent is carbon disulfide, chloroform , dichloromethane or toluene; the substrate is silicon wafer, glass, gold wafer, silver wafer, polyester film or polyimide film.
[0015] The polymer described is double-terminated polystyrene, namely B-PS n -A, see structural formula I,
[0016] .
[0017] The B terminal group in the double-terminal polystyrene is hydrophobic, and it is any one of a straight-chain alkyl group containing 4 to 21...
Embodiment 1
[0021] Octafluoro-terminated / diethylene glycol amine-terminated polystyrene (polymerization degree 50, B5-PS 50 -A2) is a film-forming polymer, dissolved in carbon disulfide to prepare a homogeneous solution with a concentration of 8 mg / mL, coated on the surface of polyester film, placed in a normal temperature atmosphere with a relative humidity of 85%, and allowed to stand for 1 minute. After the solvent is completely volatilized, a honeycomb membrane with a nanoscale pore diameter is prepared, and the pore diameter is about 45 nanometers.
Embodiment 2
[0023] Octafluoro-terminated / ethanolamine-terminated polystyrene (degree of polymerization 50, B5-PS 50 -A1) is a film-forming polymer, dissolved in carbon disulfide to prepare a homogeneous solution with a concentration of 14 mg / mL, coated on the surface of the polyester film, placed in a normal temperature atmosphere with a relative humidity of 90%, and allowed to stand for 1 minute. After the solvent is completely volatilized, a honeycomb membrane with a nanoscale pore diameter is prepared, and the pore diameter is about 75 nanometers.
PUM
Property | Measurement | Unit |
---|---|---|
Aperture | aaaaa | aaaaa |
Aperture | aaaaa | aaaaa |
Aperture | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com