Collophanite reverse flotation depressing agent and application thereof
A reverse flotation and depressant technology, applied in flotation, solid separation, etc., can solve the problems of equipment calcium accumulation and pipeline blockage, low recovery rate, low selectivity, etc., to overcome calcium accumulation and pipeline blockage, reduce Mineral dressing cost, good product quality effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0028] Weigh P 2 o 5 100g of industrial phosphoric acid with a mass percentage of 20% and P 2 o 5 400g of phosphorus pentoxide powder (oxide of yellow phosphorus) with a mass percentage of 95%.
[0029] Stir and heat industrial phosphoric acid to 90°C with a stirring speed of 1000r / min, continuously add phosphorus pentoxide powder, add 400g of phosphorus pentoxide powder in 0.5h, and stir for 1.0h to obtain collophanite reverse flotation inhibition agent.
[0030] Configure the above inhibitors into 5g / L aqueous solution for P 2 o 5 The grade is 25.35%, and the MgO content is 2.73% in the forward and reverse flotation of phosphate rock. After the raw ore is ground, the foam product is obtained through direct flotation. Add 2.5kg / t of raw ore sulfuric acid as a pH regulator to the foam, and stir for 2 minutes. Then add the inhibitor aqueous solution prepared by the above method, the inhibitor dosage is 1.5kg / t raw ore, stir for 2 minutes, do not add collector, carry out f...
Embodiment 2
[0036] Weigh P 2 o 5 100g of industrial phosphoric acid and P with a mass percentage of 40% 2 o 5 200g of phosphorus pentoxide powder (oxide of yellow phosphorus) with a mass percentage of 95%.
[0037] Stir and heat the industrial phosphoric acid to 100°C, the stirring speed is 900r / min, continue to add phosphorus pentoxide powder, add 200g of phosphorus pentoxide powder in 0.5h, stir for 45min and then get collophanite reverse flotation inhibitor .
[0038] Configure the above inhibitors into 6g / L aqueous solution for P 2 o 5 The grade is 27.33%, and the MgO content is 6.19% in the direct and reverse flotation of phosphate rock. After the raw ore is ground, the foam product is obtained through direct flotation, and 5.0kg / t of raw ore sulfuric acid is added to the foam as a pH regulator, and stirred for 2 minutes. Add the inhibitor aqueous solution prepared by the above method again, the inhibitor consumption is 1.0kg / t raw ore, stir 2min, add the fatty acid anion type ...
Embodiment 3
[0044] Weigh P 2 o 5 The mass percentage content of 85% industrial phosphoric acid 100g and P 2 o 5 100g of phosphorus pentoxide powder (oxide of yellow phosphorus) with a mass percentage of 95%.
[0045] Stir and heat the industrial phosphoric acid to 110°C, the stirring speed is 800r / min, continue to add phosphorus pentoxide powder, add 100g of phosphorus pentoxide powder in 0.5h, stir for 30min and then get the reverse flotation inhibitor of collophanite .
[0046] Configure the above inhibitors into 10% g / L aqueous solution for P 2 o 5 The grade is 25.11%, and the MgO content is 3.46% in the forward and reverse flotation of phosphate rock. After the raw ore is ground, the foam product is obtained through direct flotation. Add 3.6kg / t of raw ore sulfuric acid as a pH regulator to the foam, and stir for 2 minutes. Add the inhibitor aqueous solution that above-mentioned method prepares again, inhibitor consumption is 1.33kg / t raw ore, stirs 2min, and adding consumption ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com