Method for preventing rabbit hair fabrics from hair shedding
A technology for preventing hair loss and rabbit hair, applied in animal fibers, textiles and papermaking, fiber processing and other directions, it can solve problems such as the limitation of application scope, and achieve the effects of reducing mutual slippage, long-lasting function, and reducing hair loss rate.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0021] Example 1: A method for preventing shed hair from rabbit fur fabric, which is processed according to the following steps:
[0022] Rabbit fur surface pretreatment: soak the rabbit fur fabric to be treated in a sulfuric acid solution with a mass fraction of 2%, bath ratio 1:50, pretreatment at 60℃ for 5 min, rinse with distilled water to pH 7, and dry treatment at 60℃ 120min.
[0023] Rabbit hair graft modification: mix 2% sucrose fatty acid ester glycidyl ether of rabbit hair fabric, 2% milk protein, 2% O-9 flat and O, control pH value of 7, rabbit hair The bath ratio of the fabric to the mixed solution is 1:50. The rabbit fur fabric is water bathed at 60°C for 40 minutes; dried at 60°C for 120 minutes, and then baked and grafted at 100°C for 20 minutes. Wash the baked rabbit fur fabric three times with water, and then bake it at 60°C for 120 minutes.
Embodiment 2
[0024] Example 2: A method for preventing shed hair from rabbit fur fabric, which is processed according to the following steps:
[0025] Rabbit fur surface pretreatment: soak the rabbit fur fabric to be treated in 0.5% sulfuric acid solution, bath ratio 1:50, pretreatment at 60℃ for 2 min, rinse with distilled water to pH 8, and dry treatment at 60℃ 110min.
[0026] Rabbit hair graft modification: mix 0.5% sucrose fatty acid ester glycidyl ether of rabbit hair fabric, 0.5% sericin, 0.5% O-10 flat and O, control the pH value of 8, rabbit The bath ratio of the wool fabric to the mixed solution is 1:50. The rabbit wool fabric is dried in a water bath at 60°C for 35 minutes; dried at 60°C for 110 minutes, and then baked and grafted at a temperature of 90°C for 20 minutes. Wash the baked rabbit fur fabric 4 times with water, and then bake it at 60°C for 120 minutes.
Embodiment 3
[0027] Example 3: A method for preventing shed hair from rabbit fur fabric, which is processed according to the following steps:
[0028] Rabbit fur surface pretreatment: soak the rabbit fur fabric to be treated in 5% sulfuric acid solution, bath ratio 1:50, pretreatment at 60℃ for 2 min, rinse with distilled water to pH 6, and dry treatment at 60℃ 130min.
[0029] Rabbit hair grafting modification: mix 0.5% sucrose fatty acid ester glycidyl ether of rabbit hair fabric, 5% collagen, 5% O-20 type flat and O, control pH value of 6, rabbit hair The bath ratio of the fabric to the mixed solution is 1:50. The rabbit fur fabric is water bathed at 60°C for 35 minutes; dried at 60°C for 130 minutes, and then baked at 110°C for 20 minutes. Wash the baked rabbit fur fabric 5 times with distilled water, and then bake it at 60°C for 120 minutes.
[0030] From figure 1 with figure 2 It can be seen that before the treatment, the surface of the rabbit fur fabric was a smooth scaly layer; after t...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com