A rare earth flexible magnetic strip for health care bedding and its preparation method
A flexible magnetic strip and flexible magnet technology, which is applied in the direction of inductance/transformer/magnet manufacturing, permanent magnets, magnetic objects, etc., can solve the problem of difficulty in meeting the needs of health care bedding, low surface magnetic induction intensity, unfavorable preparation of flexible bonded magnets with magnetic properties, etc. problem, to achieve the effect of not easy to drop magnetic powder, strengthen anti-aging ability, and increase flexibility
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0062] (1) Anti-rust oil treatment: immerse 75 parts by weight of anisotropic NdFeB and NdFeN rare earth composite permanent magnet powder mixed in a mass ratio of 1:1 in 50 parts of F20-1 anti-rust oil produced by Suzhou Runtian Special Oil Co., Ltd. In the rust oil, then evacuate until the vacuum degree is -0.02MPa, and then carry out microwave treatment, the microwave frequency is 100MHz, and the microwave treatment time is 0.5min;
[0063] (2) Pre-magnetization and microwave granulation: Mix the rare earth composite permanent magnet powder treated with anti-rust oil with 4 parts of polyvinylidene fluoride, chlorinated polyethylene and ethylene-propylene rubber in a mass ratio of 1:1:1 to form The binder, 1 part of heat stabilizer, 0.5 part of coupling agent, and 0.2 part of antioxidant solution are mixed uniformly in a banbury mixer, and then pre-magnetized in a pulsed magnetic field, followed by microwave vacuum drying, specifically vacuumizing To vacuum degree is-0.02MPa...
Embodiment 2
[0070] (1) Anti-rust oil treatment: 88 parts by weight of anisotropic NdFeB and SmFeN rare earth composite permanent magnet powder mixed in a mass ratio of 1:1 were immersed in 150 parts of F20-1 anti-rust oil produced by Suzhou Runtian Special Oil Company. In the rust oil, then vacuumize until the vacuum degree is -0.001MPa, and then carry out microwave treatment, the microwave frequency is 350MHz, and the microwave treatment time is 2min;
[0071] (2) Pre-magnetization and microwave granulation: Mix the rare earth composite permanent magnet powder treated with anti-rust oil with 15 parts of ethylene-propylene rubber, 5 parts of heat stabilizer, 2 parts of coupling agent, and 0.8 parts of antioxidant solution in banburying Mix evenly in the machine, then pre-magnetize in a pulsed magnetic field, then carry out microwave vacuum drying, specifically vacuumize to a vacuum degree of -0.001MPa, and then carry out microwave treatment, the microwave frequency is 350MHz, and the micro...
Embodiment 3
[0076] (1) Anti-rust oil treatment: immerse 80 parts by weight of anisotropic NdFeB, NdFeN and SmFeN rare earth composite permanent magnet powder mixed in a mass ratio of 1:1 in 100 parts of KG-1 type quick-drying long-term anti-rust oil , and then evacuate to a vacuum degree of -0.01MPa, and then carry out microwave treatment, the microwave frequency is 200MHz, and the microwave treatment time is 1min;
[0077] (2) Pre-magnetization and microwave granulation: The rare earth composite permanent magnet powder treated with anti-rust oil was mixed with 10 parts of chlorinated polyethylene, 4 parts of heat stabilizer, 1 part of coupling agent, and 0.5 part of antioxidant solution in a dense Mix evenly in the mill, then pre-magnetize in a pulsed magnetic field, and then carry out microwave vacuum drying, specifically vacuumize to a vacuum degree of -0.008MPa, and then carry out microwave treatment, the microwave frequency is 250MHz, and the microwave treatment time is 1min. Agglome...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com