[0010] Aluminum alloy for air-conditioning radiator fins, the weight percentage of its constituent elements is: Si5.3-5.6, Fe1.2-1.4, Cu0.8-1.0, Mn2.1-2.3, Mg1.4-1.6, Cr4 .5-4.8, Zn0.2-0.4, Nb0.06-0.08, V0.5-0.6, Zr0.16-0.19, Li0.2-0.4, and the balance is aluminum.
[0011] A method for manufacturing aluminum alloys for air-conditioning radiator fins, including smelting, slag removal, alloy composition detection and adjustment, refining with refining agent, casting, including smelting, slag removal, alloy composition detection and adjustment, refining, and casting, characterized in that : After casting, cool down to 480-540°C at a rate of 110-120°C / hour and store for 1-2 hours; then cool down to 260-270°C at a rate of 130-150°C / hour and keep warm for 2-3 hours; Heat at 50-70°C / hour to 480-520°C and hold for 2-3 hours; then cool at 40-60°C / hour to 120-140°C and hold for 14-16 hours; then heat at 120-140°C / hour Heat up to 280-310°C at a rate of 2-3 hours; then cool to room temp...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com