Preparation method of catalyst for catalyzing ozonation for advanced treatment of coal chemical wastewater
A coal chemical wastewater and advanced treatment technology, applied in the direction of catalyst activation/preparation, oxidized water/sewage treatment, physical/chemical process catalysts, etc., can solve the problems of poor water solubility and low degradation rate of ozone, and achieve low cost, good physical Effect of improving structure and biodegradability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
specific Embodiment approach 1
[0023] Embodiment 1: In this embodiment, the preparation method of catalyst for advanced treatment of coal chemical industry wastewater by catalytic ozonation is carried out according to the following steps:
[0024] 1. Wash activated carbon particles with a particle size of 2-3nm until the pH value of the washing solution does not change, and then dry at 105-110°C for 5 hours;
[0025] 2. Immerse the activated carbon treated in step 1 in the metal nitrate solution, the ratio of activated carbon to the metal nitrate solution is 1:20, the concentration of the metal nitrate solution is 0.05mol / L, and then 180-200 rpm Take out the activated carbon after oscillating at a certain speed and mixing for 12 hours;
[0026] 3. Put the activated carbon into the muffle furnace after drying at 105-110°C, use nitrogen as the protective gas, first heat up to 200°C, roast for 1 hour, continue to heat up to 600°C, and roast at 600°C for 3 hours to obtain The catalyst for the advanced treatmen...
specific Embodiment approach 2
[0028] Specific embodiment two: the difference between this embodiment and specific embodiment one is that the metal nitrate solution described in step two is ferric nitrate solution, copper nitrate solution, manganese nitrate solution, aluminum nitrate solution, chromium nitrate solution, zinc nitrate solution one or a combination of several. Others are the same as in the first embodiment.
[0029] In the present embodiment, when the metal nitrate solution is a composition, the ratios between the components are arbitrary.
specific Embodiment approach 3
[0030] Embodiment 3: This embodiment differs from Embodiment 1 or Embodiment 2 in that in step 1, drying is performed at 108° C. for 5 hours. Others are the same as those in the first or second embodiment.
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com