A processing method and technology for antibacterial fabrics, applied in the field of fabric processing, can solve the problems of low antibacterial effect and washability, shorten the service life of functional fabrics, etc., and achieve long antibacterial aging, good washing resistance, and good antibacterial health effects. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] A processing method for an antibacterial fabric, comprising the following process steps:
[0019] 1) Weaving, weaving with warp and weft; the warp is made of low-twist composite yarn twisted with 28 parts by weight of nano-bamboo carbon fiber and 67 parts by weight of polyester fiber, and the warp density is 53.7 pieces / cm; The low-twisted composite yarn twisted with 38 parts by weight of nano-silver fiber and 79 parts by weight of polyester fiber is a raw material, and the weft density is 22.7 pieces / cm;
[0020] 2) Turn over the seam head;
[0021] 3) Place the cloth in 1.3G / L amylase for 58 minutes at a temperature of 87°C;
[0022] 4) Pile the cloth in 1.4G / L desizing enzyme, add 3.5g / L salt, and refine for 118 minutes;
[0023] 5) Put the cloth in 4.2G / L catalase for oxygen bleaching for 67 minutes at a temperature of 81°C;
[0024] 6) Dye the cloth again, add 17g / L sodium chloride solution to the dye, and use 2.8% acetic acid to adjust the pH value to 4.8, the ...
Embodiment 2
[0030] A processing method for an antibacterial fabric, comprising the following process steps:
[0031] 1) Weaving, weaving with warp and weft; the warp is made of low-twist composite yarn twisted with 20 parts by weight of nano-bamboo carbon fiber and 60 parts by weight of polyester fiber, and the warp density is 52.2 pieces / cm; The low-twisted composite yarn that adopts 35 parts by weight of nano-silver fibers and 75 parts by weight of polyester fibers to be twisted is a raw material, and the weft density is 21.4 pieces / cm;
[0032] 2) Turn over the seam head;
[0033] 3) Put the cloth in 0.9G / L amylase for 50 minutes at a temperature of 85°C;
[0034] 4) Pile the cloth in 0.8G / L desizing enzyme, add 3g / L salt, and refine for 110 minutes;
[0035] 5) Put the cloth in 3G / L catalase for oxygen bleaching for 65 minutes at a temperature of 72°C;
[0036] 6) Dye the cloth again, add 17g / L sodium chloride solution to the dye, and use 2.8% acetic acid to adjust the pH value to ...
Embodiment 3
[0042] A processing method for an antibacterial fabric, comprising the following process steps:
[0043] 1) Weaving is made of warp and weft; the warp is made of low-twist composite yarn twisted with 30 parts by weight of nano-bamboo carbon fiber and 75 parts by weight of polyester fiber, and the warp density is 56.1 pieces / cm; The low-twist composite yarn that adopts 45 parts by weight of nano-silver fibers and 85 parts by weight of polyester fibers to be twisted is a raw material, and the weft density is 23.7 pieces / cm;
[0044] 2) Turn over the seam head;
[0045] 3) Place the cloth in 1.5G / L amylase for 60 minutes at a temperature of 95°C;
[0046] 4) Pile the cloth in 1.7G / L desizing enzyme, add 4g / L salt, and refine for 125 minutes;
[0047] 5) Put the cloth in 5G / L catalase for oxygen bleaching for 83 minutes at a temperature of 84°C;
[0048] 6) Dye the cloth again, add 17g / L sodium chloride solution to the dye, and use 2.8% acetic acid to adjust the pH value to .3,...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com