[0023] Preparation of lithium-rich cobalt lithium manganate nanopowder
[0024] With titanium sheet as the substrate and working electrode, and graphite as the counter electrode, cobalt manganese oxide is deposited on the substrate by electrodeposition. The electrodeposition solution includes cobalt chloride with a concentration of 0.3mol / L, cobalt chloride with a concentration of 0.3mol / L manganese nitrate.
[0025] The obtained cobalt-manganese oxide and lithium chloride are miscible in water, so that the concentrations of cobalt-manganese oxide and soluble lithium salt are 15g / L and 50g / L respectively, heated to 260°C, kept at a constant temperature for 6h, centrifuged, washed, and dried to obtain Lithium cobalt manganese oxide powder.
[0026] The obtained lithium cobalt manganese oxide powder and lithium chloride are miscible in water, so that the concentrations of lithium cobalt manganese oxide and lithium chloride are respectively 10g / L and 40g / L, heated to 260°C, kept...
Embodiment 2
[0034] Preparation of lithium-rich cobalt lithium manganate nanopowder
[0035] With titanium sheet as the substrate and working electrode, and graphite as the counter electrode, cobalt manganese oxide is deposited on the substrate by electrodeposition. The electrodeposition solution includes cobalt chloride with a concentration of 0.5mol / L, and cobalt chloride with a concentration of 0.5mol / L. manganese nitrate.
[0036] The obtained cobalt-manganese oxide and lithium chloride are miscible in water, so that the concentrations of cobalt-manganese oxide and soluble lithium salt are 30g / L and 80g / L respectively, heated to 300°C, kept at a constant temperature for 4h, centrifuged, washed, and dried to obtain Lithium cobalt manganese oxide powder.
[0037] The obtained lithium cobalt manganese oxide powder and lithium chloride are miscible in water, so that the concentrations of lithium cobalt manganese oxide and lithium chloride are 15g / L and 60g / L respectively, heated to 300°C,...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com