Block polymer capable of being used as white board pen ink dispersing agent and white board pen ink
A technology of block polymers and block copolymers, applied in inks, applications, household appliances, etc., can solve problems such as limited improvement in color and luster, failure to consider environmental protection issues, and failure to specify the name of polymer dispersants, etc. Achieve the effects of easy industrialization and simple preparation process
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0042] A kind of preparation method that can be used as the block polymer of white board pen ink dispersant comprises the following steps:
[0043] In a 100ml round bottom flask, add 10g (100mmol) methyl methacrylate, 0.225g (1mmol) monomethoxyethylene glycol 2-bromoisobutyrate, 0.8173g (2mmol) 4,4'-dinonyl base-2,2'-bipyridine and 10ml of toluene, the reaction system was stirred and dissolved, and argon was bubbled for 30min, and then deoxygenated, and then the reaction system was transferred to a 100ml container containing 0.143g (1mmol) cuprous bromide In a round-bottomed flask, carry out a polymerization reaction at 90°C for 8 hours, pass the reaction product through a neutral alumina column, vacuum-dry it, and then vacuum-dry it at 40°C for 24 hours to constant weight to obtain a polymethyl methacrylate homopolymer PMMA -Br.
[0044] The results of spectral analysis of the product are as follows: 1 H-NMR (hexafluorobenzene / CDCl 3 =2 / 1 volume ratio): 3.60 (m, -O-CH 3 ,...
Embodiment 2
[0052] A kind of preparation method that can be used as the block polymer of white board pen ink dispersant comprises the following steps:
[0053] At -78°C (dry ice acetone bath), 0.19 ml (1.09 mmol) of 1,1-diphenylethylene was added to a three-necked flask containing 250 ml of anhydrous tetrahydrofuran, followed by 0.6 ml of 1.4 mol / L para Butyllithium in hexane. After 15 minutes, 9.38 g (90 mmol) of styrene was added, and after 2 hours of polymerization, 7.07 g (45 mmol) of dimethylaminoethyl methacrylate was added, and after the polymerization continued for 2 hours, 1.0 ml of anhydrous Methanol terminates the polymerization. After the reaction system was heated to 23°C, it was concentrated to 100 ml by distillation under reduced pressure, and then the polymer was precipitated in excess n-hexane, centrifuged, and freeze-dried to obtain a block copolymer containing both lipophilic and hydrophilic segments .
[0054] The characterization results of the polymer by gel exclu...
Embodiment 3
[0061] A preparation method for whiteboard pen ink, comprising the following steps:
[0062] (1) Add 0.3g PMMA 86 -b-PGMA 73 Dissolve in 3ml of acetone, then add 0.6g of carbon black therein, stir to disperse, and then remove the solvent. Then 1 g of the obtained solid powder was dispersed in 2 ml of ethanol to prepare A liquid.
[0063] (2) Dissolve 1 g of hydroxypropyl methylcellulose, 0.5 ml of glycerin, and 0.5 ml of IPP (isocaprylate) in 50 ml of ethanol, seal it, and stir until dissolved to prepare liquid B.
[0064] (3) Slowly add liquid B dropwise into liquid A, and stir to obtain the finished whiteboard pen ink.
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
dispersity | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com