A technology of antibacterial agent and zeolite, which is applied in the field of preparation of zeolite silver-loaded antibacterial agent and its liquid-phase ion exchange, can solve the problems of high loading cost, product discoloration, and influence on product appearance, and achieve high stability, cost saving, and improvement The effect of mechanical properties
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0028] Embodiment 1: direct exchange method
[0029] First carry out sodium treatment on natural clinoptilolite; weigh silver nitrate and zeolite respectively according to the ratio of silver content in zeolite material to 5%, accurately weigh a certain amount of sodium-type zeolite powder, and add concentration of 0.1mol / L respectively AgNO 3 solution (with AgNO 3 solution with a brown volumetric flask), and keep the solid-liquid ratio constant to make it fully carry out ion exchange (Ag + Avoid exposure to light during ion exchange), and adjust the pH value to 6.0-8.0 with dilute nitric acid and NaOH solution. After fully reacting, wash the silver-loaded zeolite with a centrifugal separator, and wash with distilled water until there is no Ag in the lotion. + , that is, drop in dilute hydrochloric acid without white precipitate; the exchanged zeolite is dried in an oven, and then ground and stored (the silver-exchanged zeolite should be protected from light).
Embodiment 2
[0030] Embodiment 2: indirect exchange method
[0031] First carry out sodium treatment on natural clinoptilolite; weigh silver nitrate and zeolite respectively according to the ratio of silver content in zeolite material to 5%, accurately weigh a certain amount of sodium-type zeolite powder, and add concentration of 0.1mol / L respectively NH 4 NO 3 In the solution, keep the solid-liquid ratio constant to make it fully ion-exchange, NH 4 + Substituting metal cations to form NH-loaded 4 + Zeolite, then add AgNO 3 solution, for NH 4 + with Ag + Ion exchange, and adjust the pH value to 6.0-8.0 with dilute nitric acid and NaOH solution. After fully reacting, wash the silver-loaded zeolite with a centrifugal separator, and wash it with distilled water until there is no Ag in the lotion. + , that is, drop in dilute hydrochloric acid without white precipitate; the exchanged zeolite is dried in an oven, and then ground and stored (the silver-exchanged zeolite should be protect...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com