Mixed fuel for blast furnace injection

A mixed fuel and blast furnace technology, applied in the field of metallurgy, can solve the problems of fluctuations in volatile components and reduce production costs, and achieve the effects of increased combustion rate, reduced costs, and low explosiveness

Inactive Publication Date: 2012-04-11
INNER MONGOLIA BAOTOU STEEL UNION
View PDF11 Cites 12 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0003] In order to solve the deficiencies in the existing blast furnace injection fuel technology, the present invention develops a new mixed coal with medium volatile content, which can replace the currently used anthracite and bituminous coal, so that the volatile content of pulverized coal can reach the optimum level required for blast furnace smelting. State, overcome the defects of fluctuations in volatile components caused by fluctuations in the ratio of two or more types of coal, greatly reduce production costs, and open up new coal source reserves for blast furnace coal injection

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0013] After the low-temperature semi-coke and anthracite are mixed evenly, they are pulverized into coal powder with an average particle size of 20-30 μm by a coal mill, which becomes the mixed fuel for blast furnace injection. The weight of the low-temperature semi-coke accounts for 60% of the weight of the mixed coal, and the weight of the anthracite accounts for 40% of the weight of the mixed coal.

Embodiment 2

[0015] After the low-temperature semi-coke and anthracite are mixed evenly, they are pulverized into coal powder with an average particle size of 20-30 μm by a coal mill, which becomes the mixed fuel for blast furnace injection. The weight of the low-temperature semi-coke accounts for 65% of the weight of the mixed coal, and the weight of the anthracite accounts for 35% of the weight of the mixed coal.

Embodiment 3

[0017] After the low-temperature semi-coke and anthracite are mixed evenly, they are pulverized into coal powder with an average particle size of 20-30 μm by a coal mill, which becomes the mixed fuel for blast furnace injection. The weight of the low-temperature semi-coke accounts for 70% of the weight of the mixed coal, and the weight of the anthracite accounts for 30% of the weight of the mixed coal.

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

PropertyMeasurementUnit
Average particle sizeaaaaaaaaaa
Login to View More

Abstract

A mixed fuel for blast furnace injection belongs to the technical field of metallurgy. The average particle size of mixed coal is not more than 30 microns, and the mixed coal comprises low-temperature semi coke, and anthracite; the weight of the low-temperature semi coke accounts for 60-85% of the weight of the mixed coal, and the weight of the anthracite accounts for 15-40% of the weight of the mixed coal. The low-temperature semi coke is mixed with the anthracite, which neutralizes the low-temperature semi coke with a medium volatile content. The mixed coal has low explosibility, meets the requirements for coal injection safety, increases the ratio of medium volatile bituminite to a level of 85%, greatly decreases the ratio of expensive anthracite, and thus significantly reduces the cost. The mixed coal can be used as a fuel for blast furnace injection, and has a significantly increased combustion rate level.

Description

technical field [0001] The invention relates to a mixed fuel injected into a blast furnace, which belongs to the technical field of metallurgy. Background technique [0002] In order to meet the needs of blast furnaces to reduce the coke ratio, increasing the coal ratio is the primary task. With the increase of coal injection ratio and changes in the coal market, anthracite resources are increasingly tight, and the price of anthracite will show a trend of substantial growth. Reduce the proportion of anthracite in the mixed fuel and increase the amount of cheap bituminous coal. At present, the new coal injection system is affected by factors such as fluctuations in the oxygen content of the atmosphere, and the bituminous coal ratio level is equivalent to that of the old system, which is maintained at 35-40%, which cannot fully utilize the advantages of bituminous coal injection. Chinese patent "mixed fuel injected into the blast furnace" (application number: 200910312386.9)...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
IPC IPC(8): C10L5/00
Inventor 杜国萍邬虎林赵彬韩淑霞王雅军张永高志国
Owner INNER MONGOLIA BAOTOU STEEL UNION
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products