Permeable brick and its preparation method
A technology of permeable bricks and permeable coefficient, which is applied to pavements, roads, pavements and other directions paved with prefabricated blocks. , the effect of a simple manufacturing method
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0034] 100 grams of quartz sand with a particle diameter of 0.1-0.25 mm, 4.6 grams of hydrogenated bisphenol A epoxy resin (purchased from Wuhan Shizishan Paint Factory), 1.4 grams of aliphatic polyamine curing agent (purchased from Yuanhong) Applied Materials Co., Ltd., model H-3528), 0.12 grams of γ-glycidoxypropoxypropyltrimethoxysilane (purchased from Beijing Shenda Fine Chemical Co., Ltd., model A-187), After mixing 0.012 g of light stabilizer UV-320 and 0.006 g of antioxidant 1010, 1 g of perlite powder and 3 g of alcohol, they are filled into the mold to form a permeable surface layer;
[0035] 100 grams of quartz sand with a particle diameter of 0.2-0.5 mm, 3.8 grams of hydrogenated bisphenol A epoxy resin (purchased from Wuhan Shizishan Paint Factory), 1.2 grams of aliphatic polyamine curing agent (purchased from Yuanhong Applied Materials Co., Ltd., model H-3528), 0.1 g of glycidoxypropyltrimethoxysilane (purchased from Beijing Shenda Fine Chemical Co., Ltd., model A-18...
Embodiment 2
[0038] The water-permeable brick body was prepared according to the method of Example 1, except that the quartz sand of the water-permeable surface layer was replaced by quartz sand with a particle diameter of 0.4-0.8 mm to make the water-permeable brick body.
[0039] On the surface of the main body of the prepared permeable brick, with 350g / m 2 Spray the water-based fluorocarbon paint (Beijing Zhitu Chemical, water-based fluorocarbon emulsion ZT-302) with the amount used, and then dry it at 80°C for 6 hours to make permeable bricks. After calculating the adhesion amount of the stain-resistant coating layer of the permeable brick is 200g / m 2 .
Embodiment 3
[0041] The water-permeable brick body was prepared according to the method of Example 1, except that the quartz sand of the water-permeable surface layer was replaced by quartz sand with a particle diameter of 0.2-0.45 mm to make the water-permeable brick body.
[0042] On the surface of the main body of the prepared permeable bricks, 193g / m 2 Spray the solvent-based fluorocarbon liquid (Beijing Beimu New Material, 881-Y11 fluorocarbon paint) with the amount used, and then dry it at 60°C for 4 hours to make permeable bricks. After calculation, the adhesion amount of the stain-resistant coating layer of the permeable brick is 110g / m 2 .
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com