Novel wood plastic anticorrosive wallboard and production method thereof
A production method and wood-plastic technology, applied in construction, building structure, covering/lining, etc., can solve the problems of affecting appearance, ugly products, inconvenient cleaning, etc., and achieve good effect, good printing effect and convenient installation
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0019] Embodiment 1: get 100 parts of recycled materials of PE plastics, 150 parts of bamboo powder, 10 parts of calcium carbonate, 10 parts of coupling agent, 12 parts of lubricant, 3 parts of antiaging agents, 5 parts of antibacterial agents, appropriate amount of colorant, The above raw materials are mixed, the mixing temperature is 120°C, the mixing time is 15 minutes, and the mixing speed is 700 rpm.
[0020] The above mixed wood-plastic compound is granulated through a parallel twin-screw extruder, the temperature is set at 110° C. to 200° C., and the screw speed is 150 revolutions.
[0021] The above-mentioned granulated material is extruded through a conical twin-screw extruder connected to a die, and the extrusion temperature is set at 130°C to 200°C. After cooling and shaping, it is cut to obtain two longitudinal long sides that are locked and snapped. Structural substrate.
[0022] The above-mentioned substrate is subjected to surface grinding treatment with a grin...
Embodiment 2
[0024] Embodiment 2: get 100 parts of recycled materials of PP plastics, 150 parts of wood flour, 8 parts of calcium carbonate, 10 parts of coupling agent, 12 parts of lubricant, 3 parts of antiaging agent, 5 parts of antibacterial agent, appropriate amount of coloring agent, The above raw materials are mixed, the mixing temperature is 120°C, the mixing time is 15 minutes, and the mixing speed is 700 rpm.
[0025] The above mixed wood-plastic compound is granulated through a parallel twin-screw extruder, the temperature is set at 140°C to 200°C, and the screw speed is 150 rpm.
[0026] The above-mentioned granulated material is extruded through a conical twin-screw extruder connected to a die, and the extrusion temperature is set at 160°C to 200°C. After cooling and shaping, cutting, the two longitudinal long sides are locked and snapped. Structural substrate.
[0027] The above-mentioned substrate is subjected to surface grinding treatment with a grinder.
[0028] The subst...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com