A technology for external thermal insulation and leveling mortar for external walls, applied in the direction of building and building structure, can solve the problems of cracking, low water absorption, high bonding and other problems of the external thermal insulation system, and achieves easy construction, low water absorption, and cylinder compressive strength. high effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0037] In this high-performance polyurethane external thermal insulation and anti-crack leveling mortar, the ratio of components A and B is 100:4. The amount of each substance contained in component A is: Portland cement 50kg, fly ash 11kg, expansion agent 4kg, grain Vitrified microbeads with a diameter of 30-50 mesh and a bulk density of 110-130g / L 25kg, acrylic redispersible latex powder 6kg, polycarboxylate water reducer 0.14kg, polypropylene fiber 0.27kg, polyether defoaming Agent 0.03kg, cellulose ether 0.3kg, starch ether 0.05kg, component B is epoxy modified asphalt 3.87kg.
Embodiment 2
[0039] In this high-performance polyurethane external thermal insulation and anti-crack leveling mortar, the ratio of components A and B is 100:9, and the amount of each substance contained in component A is: Portland cement 65kg, fly ash 10kg, expansion agent 5kg, granular 20kg of vitrified microbeads with a diameter of 50-70 mesh and a bulk density of 110-130g / L, 4kg of acrylic redispersible latex powder, 0.12kg of polycarboxylate water reducer, 0.03kg of polyether defoamer, polypropylene Fiber 0.25kg, cellulose ether 0.2kg, modified bentonite 0.4kg, component B is epoxy modified asphalt 9.45kg.
Embodiment 3
[0041] In this high-performance polyurethane external thermal insulation and anti-crack leveling mortar, the ratio of components A and B is 100:6, and the amount of each substance contained in component A is: ordinary Portland cement 55kg, fly ash 10kg, expansion agent 6kg, 20kg of vitrified microbeads with a particle size of 30-50 mesh and a bulk density of 110-130g / L, 9kg of vitrified microbeads with a particle size of 50-70 mesh and a bulk density of 110-130g / L, vinyl acetate redispersible latex powder 3kg, melamine water reducer 0.5kg, polyether defoamer 0.05kg, polypropylene fiber 0.3kg, cellulose ether 0.3kg, starch ether 0.05kg, modified bentonite 0.35kg, component B is epoxy Modified asphalt 6.27kg.
[0042] The high-performance polyurethane external wall thermal insulation and anti-crack leveling mortar of the present invention can be used at the construction site by mechanically adding water and stirring according to a specified ratio. It has the advantages of stabl...
PUM
Property | Measurement | Unit |
---|---|---|
particle size (mesh) | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com