Method for producing potassium chloride by using direct flotation process of third solid sylvinite
A technology of potassium chloride and potassium salt ore, which is applied in the direction of alkali metal chloride, etc., can solve problems such as limited space for expansion, and achieve the effects of saving investment and operating costs, high product purity, and high yield
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0021] Embodiment 1 A kind of method that utilizes tertiary solid potash ore positive flotation method to produce potassium chloride comprises the steps:
[0022] (1) After the raw material ore is crushed to a particle size of less than 10mm by the PE100-60 crusher produced by Wuhan Prospecting Machinery Factory, take 1080g of raw material ore and add 360g of water to decompose in the decomposition tank produced by Inner Mongolia Gold Machinery Factory. The decomposition reaction time For 25 minutes, the total potassium yield was greater than 81%, and 1440 g of slurry was obtained.
[0023] (2) The slurry is sent to the flotation process, and flotation agents and inhibitors are added respectively in the slurry, wherein the weight-to-volume ratio of raw material ore and flotation agents is 1000:0.6, and the volume ratio of flotation agents and inhibitors is 5:1; after mixing evenly, carry out flotation according to the closed-circuit process of first-stage roughing, first-stage...
Embodiment 2
[0028] Embodiment 2 A kind of method that utilizes the tertiary solid sylvitite positive flotation method to produce potassium chloride comprises the steps:
[0029] (1) After the raw ore is crushed to a particle size of less than 10mm by a crusher, 1188g of the raw ore is taken, and 360g of water is added to decompose in the decomposition tank. The decomposition reaction time is 25 minutes, and the total potassium yield is greater than 81%, obtaining 1548g of slurry .
[0030] (2) The slurry is sent to the flotation process, and flotation agents and inhibitors are added respectively in the slurry, wherein the weight-to-volume ratio of the raw material ore and the flotation agents is 1000:0.8, and the volume ratio of the flotation agents and the inhibitors is After mixing evenly, flotation is carried out according to the closed-circuit process of primary roughing, primary sweeping, and secondary beneficiation, with a total of 5 minutes of flotation, and 136g of flotation conce...
Embodiment 3
[0035] Embodiment 3 A kind of method utilizing the tertiary period solid potash ore positive flotation method to produce potassium chloride comprises the following steps:
[0036] (1) After the raw material ore is crushed to a particle size less than 10mm by a crusher, 1152g of the raw material ore is taken, and 360g of water is added to decompose in a decomposition tank. The decomposition reaction time is 25 minutes, and the total potassium yield is greater than 81%, obtaining 1512g of slurry .
[0037] (2) The slurry is sent to the flotation process, and flotation agents and inhibitors are added respectively in the slurry, wherein the weight-to-volume ratio of raw material ore and flotation agents is 1000:0.7, and the volume ratio of flotation agents and inhibitors is 5.5:1; after mixing evenly, carry out flotation according to the closed-circuit process of first-stage roughing, first-stage sweeping, and second-stage beneficiation, for a total of 5 minutes of flotation, and ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com