Medical security level rubber product with sericin modified surface and preparation method thereof
A rubber product and safety-grade technology, which is applied to medical safety-grade rubber products with sericin modified surface and its preparation field, can solve the problems of unsatisfactory effect, decreased strength of natural rubber, and decreased use performance, and achieves improved use. Comfort and hygienic safety, improved rubber strength, and resource-saving effects
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
example 1
[0052] The preparation of example 1-sericin
[0053] Use cocoon, waste silk, and waste as raw materials, extract it with acetone for 24 hours, remove impurities, degumming with high-temperature water solution, filter sericin aqueous solution at 80 ° C, dialysis for 4 hours, then concentrate it, freeze-dry to obtain Powdered sericin with a purity of 90% or more.
example 2
[0054] Preparation of example 2-sericin hydrolyzate
[0055] The sericin obtained above is subjected to hot water treatment, that is, in 0.2% sodium carbonate aqueous solution (pH 11-12) at 95° C. for 2-4 hours, so as to extract sericin protein hydrolyzate. The obtained sericin hydrolyzate extract was filtered through a filter with an average pore diameter of 0.3um to remove focused matter. The filtrate was then desalted through a reverse osmosis membrane to obtain a 0.3% aqueous solution of clear and colorless sericin hydrolyzate.
[0056] The solution is concentrated to a concentration of about 0.3% with an evaporator, and then freeze-dried to obtain a powder-formed sericin hydrolyzate with a purity of 90% or more and an average molecular weight of 0.1×10 4 -2.0×10 4 .
example 3
[0057] The preparation of example 3-chitosan
[0058] The crudely extracted chitin is treated with 3-6 times of 60-75% concentrated sodium hydroxide at 70-95°C for 10-20 hours for deacetylation reaction to obtain crude chitosan, and then the crude chitosan product is dissolved Add 7-10 times of 2-7% dilute acetic acid, then add 10% concentrated lye to form viscous, stand at 5-30°C for 2-6 hours, neutralize with dilute acid to pH 8- 9 until flocs appear, continuously stir until the flocs stop producing, and then remove sodium chloride to obtain water-soluble chitosan with a molecular weight of 0.5×105-0.8×105 and a degree of deacetylation of 50%-95%.
PUM
Property | Measurement | Unit |
---|---|---|
purity | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com