Examples
Embodiment 1
[0017] Y(NO 3 ) 3 6H 2 O 4.7880g, HfOCl 2 11.6110g, 0.095mol / l Eu(NO 3 ) 3 Solution 4.0ml, C 2 h 5 NO 2 0.7820g, CH 4 N 2 O 0.9384g.
[0018] Weigh 4.7880g Y(NO 3 ) 3 6H 2 O powder and 11.6110 g HfOCl 2 After the powder was put into a beaker and dissolved in distilled water, 4.0ml of Eu(NO 3 ) 3 solution, measure the pH value of the solution, and adjust it to approximately equal to 1 with nitric acid. Put the beaker on the magnetic stirrer, add 0.7820g of glycine C to it while stirring 2 h 5 NO 2 and 0.9384g urea CH 4 N 2 O, and add 0.015 g of EDTA as a chelating agent, and stir vigorously for a while until the raw material is mixed with the fuel. Put the mixture in an oven at 200°C to evaporate the water, then put it into a muffle furnace and heat it to 450°C to make it foam and burn, and then heat it in a high-temperature furnace at 800°C for 2 hours to finally get the desired Luminescent material.
[0019] Referring to the accompanying drawings, the s...
Embodiment 2
[0021] Y(NO 3 ) 3 6H 2 O 4.7880g, HfOCl 2 11.6110g, 0.095mol / l Eu(NO 3 ) 3 Solution 6.0ml, C 2 h 5 NO 2 0.7820g, CH 4 N 2 O 0.9384g.
[0022] Weigh 4.7880g Y(NO 3 ) 3 6H 2 O powder and 11.6110 g HfOCl 2 After the powder was put into a beaker and dissolved in distilled water, 6.0ml of Eu(NO 3 ) 3 solution. Measure the pH of the solution and adjust it to approximately 1 with nitric acid. Put the beaker on the magnetic stirrer, add 0.7820g of glycine C to it while stirring 2 h 5 NO 2 and 0.9384g urea CH 4 N 2 O, and add 0.015 g of EDTA as a chelating agent, and stir vigorously for a while until the raw material is mixed with the fuel. Put the mixture in an oven at 200°C to evaporate the water, then put it into a muffle furnace and heat it to 450°C to make it foam and burn, and then heat it in a high-temperature furnace at 800°C for 2 hours to finally get the desired Luminescent material. The structure of the luminescent material synthesized in this exampl...
Embodiment 3
[0024] Y(NO 3 ) 3 6H 2 O4.7880g, HfOCl 2 11.6110g, 0.095mol / l Eu(NO 3 ) 3 Solution 8.0ml, C 2 h 5 NO 2 0.7820g, CH 4 N 2 O0.9384g.
[0025] Weigh 4.7880g Y(NO 3 ) 3 6H 2 O powder and 11.6110 g HfOCl 2 After the powder was put into a beaker and dissolved in distilled water, 8.0ml of Eu(NO 3 ) 3 solution. Measure the pH of the solution and adjust it to approximately 1 with nitric acid. Put the beaker on the magnetic stirrer, add 0.7820g of glycine C to it while stirring 2 h 5 NO 2 and 0.9384g urea CH 4 N 2 O, and add 0.015 g of EDTA as a chelating agent, and stir vigorously for a while until the raw material is mixed with the fuel. Put the mixture in an oven at 200°C to evaporate the water, then put it into a muffle furnace and heat it to 450°C to make it foam and burn, and then heat it in a high-temperature furnace at 800°C for 2 hours to finally get the desired Luminescent material. The structure of the scintillation material synthesized in this example...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com