Method for preparing oilfield additive calcium bromide
The technology of an oilfield additive and calcium bromide, which is applied in the field of preparation of calcium bromide, can solve problems such as packaging, transportation and storage troubles, low yield of ferrous bromide method, affecting product quality, etc. Inexpensive, inexpensive effects
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] The method utilizing hydrobromic acid of the present embodiment to prepare oilfield additive calcium bromide adopts the following steps:
[0019] (1) Lime emulsification: Add 120kg of water to the 2000L batching tank made of glass steel, then start stirring, and slowly pour 260kg of quicklime into the batching tank until the feed liquid is evenly distributed;
[0020] (2) neutralization: gradually add the hydrobromic acid of 1360kg in batching tank, add in 35 minutes, after stirring again for 8 minutes, adjust the pH value to 6.8;
[0021] (3) Impurity treatment: 5kg of activated carbon, 10kg of activated clay and 3kg of 60-purpose chitosan leftovers were added to the above feed liquid and stirred and adsorbed for 60 minutes;
[0022] (4) Settling and filtering: after the feed liquid is put into the sedimentation tank for 4.5 hours, extract the above feed liquid into a filter press for pressure filtration, and collect the filtrate to the filtrate storage tank;
[0023]...
Embodiment 2
[0026] The method utilizing hydrobromic acid of the present embodiment to prepare oilfield additive calcium bromide adopts the following steps:
[0027] (1) Lime emulsification: Add 120kg of water to the 2000L batching tank made of glass steel, then start stirring, and slowly pour 300kg of quicklime into the batching tank until the feed liquid is evenly distributed;
[0028] (2) neutralization: gradually add the hydrobromic acid of 1620kg in batching tank, add in 45 minutes, after stirring again for 10 minutes, adjust the pH value to 6.5;
[0029] (3) Impurity treatment: 8kg of activated carbon, 12kg of activated clay and 5kg of 90-purpose chitosan leftovers were added to the above feed liquid and stirred and adsorbed for 80 minutes;
[0030] (4) Settling and filtering: after the feed liquid is put into the sedimentation tank for 5 hours, extract the above feed liquid into a filter press for pressure filtration, and collect the filtrate to the filtrate storage tank;
[0031] ...
Embodiment 3
[0034] The method utilizing hydrobromic acid of the present embodiment to prepare oilfield additive calcium bromide adopts the following steps:
[0035] (1) Lime emulsification: Add 150kg of water to the 2000L batching tank made of glass steel, then start stirring, and slowly pour 270kg of quicklime into the batching tank until the feed liquid is evenly distributed;
[0036] (2) neutralization: gradually add the hydrobromic acid of 1620kg in batching tank, add in 45 minutes, after stirring again for 10 minutes, adjust the pH value to 6.5;
[0037] (3) Impurity treatment: 7kg of activated carbon, 11kg of activated clay and 4kg of 80-purpose chitosan leftovers were added to the above feed liquid and stirred and adsorbed for 80 minutes;
[0038] Following steps are with embodiment 2, and gained liquid calcium bromide finished product, productive rate is 93.1%.
[0039] The calcium bromide product that the embodiment of the present invention gained is assayed, and the results are...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com