Therapy electrode tablet clamping self-pasting medicament film and preparation method thereof
A drug-loaded film and self-adhesive technology, which is applied in the direction of electrodes, electrotherapy, and pharmaceutical formulations, can solve the problems of reducing the adhesive performance of conductive adhesives, reducing application flexibility, and increasing production costs, so as to overcome the problem of high price, The effect of reducing the competition transmission and reducing the cost of use
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0029] 1. Preparation of buffer layer gel material
[0030] Dissolve 2 g of Carbomer 940 in 50 mL of deionized water, add 6.3 g of triethanolamine under stirring to gel the carbomer solution, while stirring, add 40 g of sodium alginate with a mass concentration of 2.5% (1% aqueous solution viscosity) About 200mPa·s) solution, 25mL pH6.5 acetate buffer solution, 2 grams of citric acid solution with a mass concentration of 15%, 18 grams of glycerol, 20 grams of polyvinyl alcohol 17-99 solution with a mass concentration of 10%, 10 Maltose with a gram mass concentration of 25%, 10 grams of sucrose with a mass concentration of 25%, 0.1 grams of sodium benzoate, and 10 grams of a potassium iodide solution with a mass concentration of 10% were added to the gel, mixed well and degassed.
[0031] 2. Preparation of the release layer gel material
[0032] Dissolve 2 g of Carbomer 940 in 50 mL of deionized water, add 4 g of triethanolamine under stirring to gel the carbomer solution, mix 1.7 ...
Embodiment 2
[0036] The preparation process of the buffer layer gel material is the same as that in Example 1, except that the pH 6.5 acetate buffer solution is changed to a pH 7.2 phosphate buffer solution.
[0037] The preparation process of the drug-releasing layer gel material is the same as that of Example 1.
[0038] The preparation process of the physiotherapy electrode sheet sandwiching the self-adhesive drug-loaded film is the same as that of Example 1. In the physical therapy electrode sheet sandwiching the self-adhesive drug-loading film, the thickness of the buffer layer is 0.5 mm and the thickness of the drug release layer It is 0.5mm.
Embodiment 3
[0040] The preparation process of the buffer layer gel material is the same as that in Example 1, except that the pH 6.5 acetate buffer solution is changed to a pH 7.6 phosphate buffer solution.
[0041] The preparation process of the drug-releasing layer gel material is the same as that of Example 1.
[0042] The preparation process of the physiotherapy electrode sheet sandwiching the self-adhesive drug-loaded film is the same as that of Example 1. In the physical therapy electrode sheet sandwiching the self-adhesive drug-loading film, the thickness of the buffer layer is 0.5 mm and the thickness of the drug release layer It is 0.5mm.
PUM
Property | Measurement | Unit |
---|---|---|
thickness | aaaaa | aaaaa |
thickness | aaaaa | aaaaa |
thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com