Tocopheryl polyethylene glycol succinate powder and process for preparing same
A technology of polyethylene glycol succinate and polyethylene glycol, applied in food preparation, powder delivery, pharmaceutical formulations, etc., can solve problems such as difficulty in taking out, increased risk of product contamination, inconvenience, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0028] This example demonstrates a method from solid TPGS TM Preparation of powdered TPGS TM Methods. Grinding Eastman Vitamin E TPGS at low temperature with a Spex Freezer / Mill TM 1000, N.F. Its purpose is to determine the range of particles obtained by cryogenic grinding.
[0029] Fill the freezing / grinding chamber with liquid nitrogen. Weigh 5 grams of vitamin ETPGS ground into pieces TM 1000, NF into a sample tube. Use a metal rod as an impactor into the TPGS TM Remove the debris from the sample tube and seal the sample tube. Put the sample into the working chamber and close the valve. Set the timer for a 6 minute run time after reducing the steam flow for about 4 minutes. The samples were removed from the chamber after six minutes and allowed to warm to room temperature. Remove TPGS from sample tube TM and particle size analysis. Primary particles are blue in color with a minimum particle size of about 0.5 microns.
Embodiment 2
[0031] This example demonstrates a method for preparing powdered TPGS from liquid material TM Methods. To 300 g of acetone was added 173 g of TPGS melting at 75°C TM . Stir this mixture until TPGS forms TM solution. Samples were spray dried using an APV Anhydro Lab Model 1 spray dryer. The atomization process used a spray dryer with 2 fluid nozzles and nitrogen as the atomizing gas. The solution was loaded into the dryer with a Masterflex pipeline pump. See Table 1 for operating conditions.
[0032] Table 1
[0033] Inlet temperature °C
23
Outlet temperature °C
20
Nitrogen Partial Pressure (δP) (in H2O)
60
Atomization pressure (psi)
45
pump speed
18
Feed weight (g)
304
Running time (minutes)
28
Feed rate (g / min)
10.8
Yield (g)
13.5
[0034] Thanks to Vitamin E TPGS TM has a low melting point so no heating was performed. TPGS obtained by spray drying TM The ave...
Embodiment 3
[0039] A 20% aqueous solution of powdered TPGS was prepared. Add 20 g of powdered TPGS to 80 g of ultrapure water at 5°C while stirring TM . Add a 4 gram serving of TPGS TM and stir until a solution forms.
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
glass transition temperature | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
![application no application](https://static-eureka-patsnap-com.libproxy1.nus.edu.sg/ssr/23.2.0/_nuxt/application.06fe782c.png)
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com