Environment-friendly water-soluble soil conditioner containing petrifaction and minerals and preparation method thereof
A soil conditioner, water-soluble technology, applied in the field of environmental protection water-soluble soil conditioner and its preparation, can solve the problems of inability to effectively precipitate a large number of elements, difficulty in improving yield and quality, low soil fertility performance, etc. Utilization, low cost of acquisition, effect of improving fertility
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0023] The preparation method of an environment-friendly water-soluble soil improver containing petrochemicals and minerals comprises the following steps: after burning petrochemical calcium, medical stone and sulfur at high temperature, adding distilled water and placing them in a reaction kettle; The electrolysis device electrolyzes; after the electrolysis process, the liquid and sludge are separated; copper sulfate pentahydrate, manganese nitrate hexahydrate, zinc sulfate heptahydrate, magnesium chloride and potassium chloride are added to the liquid, and the finished soil conditioner is obtained after bottling. Under normal circumstances, petrochemical calcium, medical stone and sulfur are directly used in the soil after being crushed, and the elements in the raw materials cannot be used by plants, and there is no improvement effect on the soil. Heating at a temperature above 220°C, followed by electrolysis, can fully dissolve a large amount of water-soluble elements, and c...
Embodiment 1
[0031] An environmentally friendly water-soluble soil conditioner containing petrochemicals and minerals, which is prepared by the following steps:
[0032] 35% by weight of petrified calcium, 3% by weight of medical stone and 2% by weight of sulfur (the mesh size is 2000 mesh) are fired at high temperature at 1100°C for 48 hours, and then 59.82% by weight is added. % of distilled water, placed in the reactor;
[0033] After the reaction kettle is heated to 230°C, keep the temperature constant for 24 hours, and then continue electrolysis at 65°C for 6.0 hours through the electrolysis device;
[0034] After the electrolysis process, the liquid and sludge are separated, and the resulting liquid contains a high concentration of calcium ions;
[0035] Add the copper sulfate pentahydrate of 0.05% by weight, the manganese nitrate hexahydrate of 0.03% by weight, the zinc sulfate heptahydrate of 0.03% by weight, the magnesium chloride of 0.03% by weight and the potassium chloride of ...
Embodiment 2
[0041] An environmentally friendly water-soluble soil conditioner containing petrochemicals and minerals, which is prepared by the following steps:
[0042] 32% by weight of petrochemical calcium, 2% by weight of medical stone and 1% by weight of sulfur (the mesh size is 1950 mesh) are fired at high temperature at 1000°C for 47 hours, and then 64.87% by weight is added. % of distilled water, placed in the reactor;
[0043] After the reaction kettle was heated to 220°C, the temperature was kept constant for 23.5 hours, and then electrolysis was continued at 60°C for 6.2 hours through the electrolysis device;
[0044] After the electrolysis process, the liquid and sludge are separated, and the resulting liquid contains a high concentration of calcium ions;
[0045] Add the copper sulfate pentahydrate of 0.04% by weight, the manganese nitrate hexahydrate of 0.02% by weight, the zinc sulfate heptahydrate of 0.02% by weight, the magnesium chloride of 0.02% by weight and the potass...
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com