[0018] An anti-graffiti and anti-scratch tempered art paint, comprising the following raw materials in parts by weight, 85-95 parts of modified organic-inorganic hybrid resin, 1-4 parts of nano-titanium dioxide, and 1-4 parts of silica, 6-12 parts of graphene, 6-10 parts of perlite, 0.5-2 parts of silane coupling agent and 0.5-3 parts of dispersant.
[0019] Take 92 parts of modified organic-inorganic hybrid resin, 2 parts of nano-titanium dioxide, 2 parts of nano-silicon dioxide, 9 parts of graphene, 7 parts of perlite, 1 part of silane coupling agent after using hydroxyfluorosilicone oil to modify the silicone material parts and 2 parts of BYK-9076 dispersant, add 20 parts of water, ultrasonically mix the components and heat for 15 minutes, the heating temperature is 70 ℃, and finally the product is obtained by cooling to room temperature.
Embodiment 2
[0021] Take 90 parts of modified organic-inorganic hybrid resin, 1 part of nano-titanium dioxide, 1 part of nano-silicon dioxide, 8 parts of graphene, 6 parts of perlite, and 0.5 parts of silane coupling agent after using hydroxyfluorosilicone oil to modify the silicone material. part and 0.5 part of BYK-9076 dispersant, add 20 parts of water, ultrasonically mix the components and heat for 15 minutes, the heating temperature is 70 ℃, and finally the product is obtained by cooling to room temperature.
Embodiment 3
[0023] Take 95 parts of modified organic-inorganic hybrid resin, 3 parts of nano-titanium dioxide, 3 parts of nano-silicon dioxide, 12 parts of graphene, 8 parts of perlite, and 2 parts of silane coupling agent after using hydroxyfluorosilicone oil to modify the silicone material. parts and 3 parts of BYK-9076 dispersant, add 20 parts of water, ultrasonically mix the components and heat for 15 minutes, the heating temperature is 70 ℃, and finally the product is obtained by cooling to room temperature.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com