A self-propelled anti-icing material based on modulus patterning and its preparation method
A self-driven, modulus technology, applied to flat products, other household appliances, coatings, etc., can solve the problems of unsustainable anti-icing effect and insufficient anti-icing performance, and achieve large-scale production and stable anti-icing performance , the effect of a wide range of raw materials
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0041] Preparation method of self-propelled anti-icing material
[0042] The self-propelled anti-icing material of the present invention can be made by various methods, and the specific method can be selected according to factors such as the scale and shape of the modulus pattern, and the properties of raw materials. Taking PDMS (polydimethylsiloxane) as the base material as an example, several optional methods are given below. The process of preparing patterns with other basic materials can be referred to.
[0043] Preparation Method 1: Heat Curing
[0044] This method is suitable for processing modulus patterned materials with a centimeter-scale scale, and it can also be selected for processing materials with other scales depending on the situation.
[0045] Step 1: Design a modulus pattern (such as bar, square, circle, etc.), and make a mold with detachable partition baffles according to the designed modulus pattern.
[0046] Step 2: Inject a specific proportion of PDM...
Embodiment 1
[0062] Mix the PDMS monomer and the curing agent at a ratio of 1:1 to obtain a precursor, stir evenly and place it in a vacuum oven to remove air bubbles at room temperature. Pour the precursor into a glass mold with a flat bottom, cure at 80°C for 2 hours, and demould for storage.
Embodiment 2
[0064] Mix the PDMS monomer and curing agent at a ratio of 20:1 to obtain a precursor, stir evenly and place it in a vacuum oven to remove air bubbles at room temperature. Pour the precursor into a glass mold with a flat bottom, cure at 80°C for 2 hours, and demould for storage.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com