A kind of wetting agent for three-proof finishing and preparation method thereof
A technology of three-proof finishing and wetting agent, applied in fiber treatment, anti-coloring pollution/anti-fouling fiber, and repelling fiber to liquid, etc. , Rapid defoaming function, low foaming effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0028] A wetting agent for three-proof finishing, in parts by mass, comprising the following raw materials: 6 parts of surfactant (LutensolON70, Pluronic PE9200, Tetronic 207, the mass ratio is 1:8:1), and the molecular formula is C 6 H 5 -O-R-OH substance (ethylene glycol phenyl ether) 10 parts, environmentally friendly solvent (diethylene glycol) 10 parts, water 74 parts.
[0029] The preparation method of the wetting agent for three-proof finishing comprises the following steps:
[0030] 1) respectively take by weighing the surfactant of formula amount, molecular formula is C 6 H 5 -O-R-OH substances, environmentally friendly solvents and water, for use;
[0031] 2) under normal temperature and pressure, add 37 parts of water in the reactor equipped with agitator, be warming up to 60 ℃, then add 6 parts of surfactants (Lutensol ON70, Pluronic PE9200, Tetronic 207, mass ratio is 1:8 : 1), and stirred for 20min;
[0032] 3) adding 10 parts of ethylene glycol phenyl ether...
Embodiment 2
[0036] A wetting agent for three-proof finishing, in parts by mass, comprising the following raw materials: 9 parts of surfactants (Lutensol ON70, Lutensol ON50, Pluronic PE6200, Tetronic 207; the mass ratio is 1:1:16:2), and the molecular formula is 15 parts of C6H5-O-R-OH substances (ethylene glycol phenyl ether), 6 parts of environmentally friendly solvents (diethylene glycol, triethylene glycol butyl ether), and 70 parts of water.
[0037] The preparation method of the wetting agent for three-proof finishing comprises the following steps:
[0038] 1) respectively take by weighing the surfactant of formula quantity, molecular formula is the material of C6H5-O-R-OH, environmental protection solvent and water, for subsequent use;
[0039]2) under normal temperature and pressure, add 35 parts of water in the reactor equipped with agitator, be warming up to 60 ℃, then add 9 parts of surfactants (Lutensol ON70, Lutensol ON50, Pluronic PE6200, Tetronic 207; mass ratio is 1:1:16:...
Embodiment 3
[0044] A wetting agent for three-proof finishing, in parts by mass, comprising the following raw materials: surfactant (Lutensol ON60, Lutensol ON50, Pluronic PE6200, Pluronic PE9200, Tetronic RED 9040; mass ratio is 1:1:16:1:1 ) 3 parts, the molecular formula is C6H5-O-R-OH substance (propylene glycol phenyl ether) 20 parts, environmental protection solvent (dipropylene glycol, triethylene glycol butyl ether; mass ratio is 1:1) 10 parts, water 67 parts.
[0045] The preparation method of the wetting agent for three-proof finishing comprises the following steps:
[0046] 1) respectively take by weighing the surfactant of formula amount, molecular formula is C 6 H 5 -O-R-OH substances, environmentally friendly solvents and water, for use;
[0047] 2) Under normal temperature and pressure, add 33.5 parts of water in the reactor equipped with agitator, heat up to 60 ° C, then add 3 parts of surfactants (Lutensol ON60, Lutensol ON50, Pluronic PE6200, Pluronic PE9200, Tetronic RE...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com