A technology of conductive ink and graphene, which is applied in the direction of ink, household utensils, applications, etc., can solve the problems of easy agglomeration of graphene and difficulty in preparing uniformly dispersed graphene composite materials, and achieve the effect of avoiding the use of toxic organic solvents
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0022] Weigh 0.5g of epoxy resin in a small beaker, add 0.1g of graphene powder at the same time, add 30ml of ethanol as a solvent, configure a dispersion, stir for 10 minutes, and ultrasonicate for half an hour; add 0.05g of it dropwise The brominated 1-vinyl-3-methylimidazole was ultrasonically treated for two hours again; polyetheramine (epoxy resin:polyetheramine=3:1) with a certain ratio to epoxy resin was added, and properly stirred to disperse , the prepared graphene conductive ink is coated on common A4 printing paper, and dried naturally to obtain the graphene conductive ink coating coated on A4 printing paper.
Embodiment 2
[0024] Weigh 0.5g of epoxy resin in a small beaker, add 0.1g of graphene powder at the same time, add 30ml of ethanol as a solvent, configure a dispersion, stir for 10 minutes, and ultrasonicate for half an hour; add 0.1g of it dropwise The brominated 1-vinyl-3-methylimidazole was ultrasonically treated for two hours again; polyetheramine (epoxy resin:polyetheramine=3:1) with a certain ratio to epoxy resin was added, and properly stirred to disperse , the prepared graphene conductive ink is coated on ordinary A4 printing paper, and dried naturally to obtain a graphene conductive ink coating coated on A4 printing paper, and the conductivity is improved.
Embodiment 3
[0026] Weigh 0.5g of epoxy resin in a small beaker, add 0.1g of graphene powder at the same time, add 30ml of ethanol as a solvent, configure a dispersion, stir for 10 minutes, and ultrasonicate for half an hour; add 0.2g of it dropwise The brominated 1-vinyl-3-methylimidazole was ultrasonically treated for two hours again; polyetheramine (epoxy resin:polyetheramine=3:1) with a certain ratio to epoxy resin was added, and properly stirred to disperse , the prepared graphene conductive ink is coated on common A4 printing paper, and dried naturally to obtain the graphene conductive ink coating coated on A4 printing paper.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com