A water-soluble composite and water-soluble polymer technology, applied in the field of composite glue, can solve the problems of slow drying speed of composite glue, poor adhesion performance, low water content, etc., and achieve good composite fastness, excellent weather resistance, The effect of low water content

Inactive Publication Date: 2019-12-31
常州天南化工有限公司
View PDF3 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0006] In view of the problems existing in the prior art, the object of the present invention is to provide a water-soluble composite glue and its preparation method, which has the advantages of less water content and good bonding performance, and solves the problem of the traditional water-soluble composite glue containing The amount of water is too much, which leads to the slow drying speed of the composite glue, and the bonding performance is not very good.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0027] A water-soluble composite glue, comprising the following raw materials in parts by weight: 30 parts of polyisocyanate, 15 parts of water-soluble polymer, 10 parts of polyol, 4 parts of emulsifier, 3 parts of stabilizer, 2 parts of initiator, 15 parts of kaolin and the balance of deionized water.

[0028] Further, the emulsifier is composed of one or more of fatty alcohol polyoxyethylene ether, alkylphenol polyoxyethylene ether, fatty acid polyol ester and alkyl sulfate.

[0029] Further, the stabilizer is composed of one or more of pectate, caseinate, methyl cellulose, carboxymethyl cellulose, polyvinyl alcohol, sodium polyacrylate and styrene-acid anhydride copolymer.

[0030] Further, the initiator is ammonium persulfate, and the water-soluble polymer is anionic polyacrylamide.

[0031] A preparation method of water-soluble composite glue, comprising the following steps:

[0032] S1. Add emulsifier, stabilizer, and kaolin into deionized water in sequence, and stir f...

Embodiment 2

[0038] A water-soluble composite glue, comprising the following raw materials in parts by weight: 40 parts of polyisocyanate, 20 parts of water-soluble polymer, 15 parts of polyol, 6 parts of emulsifier, 4.5 parts of stabilizer, 3 parts of initiator, 20 parts of kaolin and the balance deionized water.

[0039] Further, the emulsifier is composed of one or more of fatty alcohol polyoxyethylene ether, alkylphenol polyoxyethylene ether, fatty acid polyol ester and alkyl sulfate.

[0040] Further, the stabilizer is composed of one or more of pectate, caseinate, methyl cellulose, carboxymethyl cellulose, polyvinyl alcohol, sodium polyacrylate and styrene-acid anhydride copolymer.

[0041] Further, the initiator is ammonium persulfate, and the water-soluble polymer is anionic polyacrylamide.

[0042] A preparation method of water-soluble composite glue, comprising the following steps:

[0043] S1. Add emulsifier, stabilizer, and kaolin into deionized water in sequence, and stir fo...

Embodiment 3

[0049] A water-soluble composite glue, comprising the following raw materials in parts by weight: 50 parts of polyisocyanate, 25 parts of water-soluble polymer, 20 parts of polyol, 8 parts of emulsifier, 6 parts of stabilizer, 4 parts of initiator, 25 parts of kaolin and the balance of deionized water.

[0050] Further, the emulsifier is composed of one or more of fatty alcohol polyoxyethylene ether, alkylphenol polyoxyethylene ether, fatty acid polyol ester and alkyl sulfate.

[0051] Further, the stabilizer is composed of one or more of pectate, caseinate, methyl cellulose, carboxymethyl cellulose, polyvinyl alcohol, sodium polyacrylate and styrene-acid anhydride copolymer.

[0052] Further, the initiator is ammonium persulfate, and the water-soluble polymer is anionic polyacrylamide.

[0053]A preparation method of water-soluble composite glue, comprising the following steps:

[0054] S1. Add emulsifier, stabilizer, and kaolin into deionized water in sequence, and stir fo...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention belongs to the field of composite adhesives and discloses a water-soluble composite adhesive. The water-soluble composite adhesive is prepared from the following raw materials in parts by weight: 30-50 parts of polyisocyanate, 15-25 parts of water-soluble high polymer, 10-20 parts of polyol, 4-8 parts of emulsifier, 3-6 parts of stabilizer, 2-4 parts of initiator, 15-25 parts of kaolin and the balance of deionized water. The water-soluble composite adhesive disclosed by the invention is low in moisture content, high in drying speed, difficult in deformation and low in dosage andis not absorbed by adhered objects, and thus, the production cost is reduced greatly; the water-soluble composite adhesive prepared by a preparation method disclosed by the invention is stable in performance, excellent in weather resistance and good in compounding fastness; the water-soluble composite adhesive prepared by taking the polyisocyanate, the water-soluble high polymer, the polyol, the kaolin and the like as main raw materials has relatively high bond strength and impact toughness; and the kaolin has a relatively good thickening effect, so that the precipitation of the prepared water-soluble composite adhesive is avoided, and the kaolin can exert a dispersing action.

Description

technical field [0001] The invention relates to the technical field of composite glue, in particular to a water-soluble composite glue and a preparation method thereof. Background technique [0002] Composite glue is used for bonding and compounding between two or more layers of materials. It is the main raw material for the production of material packaging composite films. The composite glue can be divided into one-component glue and two-component glue, which can be divided according to the solvent used. It is traditional solvent-based adhesive, alcohol-soluble adhesive and water-soluble composite adhesive. [0003] Among them, environment-friendly composite adhesives, that is, alcohol-soluble and water-soluble composite adhesives, have become the focus of research and application at home and abroad in recent years. Traditional water-soluble composite adhesives contain a lot of water when used, resulting in slow drying of the composite adhesive and poor adhesion. The perfo...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): C09J175/04C09J11/04
CPCC09J11/04C09J175/04C08K3/346
Inventor 陈翼
Owner 常州天南化工有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products